A low SV causes relatively slow pyrolysis conditions at around 600°C, and produces high yields of charcoal 20-30%, large quantities of unburned tars, and a gas with high hydrocarbon content and high tar (volatile) content. A high SV causes very fast pyrolysis, producing less than 10% char-ash at 1050 C and hot gases at 1200-1400 C in the flaming pyrolysis zone. These gases then react with the r...