Transmission Electron Microscopy Sample Preparation of INCONEL 738 Nickel-Base Superalloy

نویسندگان

  • F. A. Hesari Materials Characterization Group, Materials and Energy Research Center, Meshkin Dasht, Karaj, Iran
  • F. S. Torknik Materials Characterization Group, Materials and Energy Research Center, Meshkin Dasht, Karaj, Iran
  • M. Moradi Materials Characterization Group, Materials and Energy Research Center, Meshkin Dasht, Karaj, Iran
چکیده مقاله:

Size, shape, volume fraction and distribution of embedded g/ phase in g phase has direct effect on strength of INCONEL alloy. Microstructure parameters of INCONEL phases are quantified from microstructure images using transmission electron microscopy (TEM). Different TEM sample preparation techniques were used to study INCONEL 738 alloy microstructure for transmission electron microscopy (TEM). The INCONEL 738 was first cut into a 1 × 1 cm slice with 600 µm thickness with diamond wire cut. INCONEL sample was mounted by wax (M135), after initial grinding and polishing. The molded INCONEL sample was further polished by different grit size SiC paper to reduce the thickness below 80 micron. At this stage, 3 mm discs were cut from the thin slice of INCONEL alloy by mechanical punch machine. The 3 mm discs of INCONEL alloy were used for TEM sample preparation. Three methods of electro-jet polishing, ion milling and micro control dimpling were employed to prepare transparent TEM sample to observe the surface microstructure details of INCONEL 738 alloy. Electro-jet polishing TEM sample preparation technique could reveal microstructure details of INCONEL alloy g and g/ phases using 42% H3PO4, 34% H2SO4, 24% H2O electrolyte at about – 400C bath temperature and applied voltage of 30 V.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

Measurement of gamma' precipitates in a nickel-based superalloy using energy-filtered transmission electron microscopy coupled with automated segmenting techniques.

Precipitates of the ordered L1(2) gamma' phase (dispersed in the face-centered cubic or FCC gamma matrix) were imaged in Rene 88 DT, a commercial multicomponent Ni-based superalloy, using energy-filtered transmission electron microscopy (EFTEM). Imaging was performed using the Cr, Co, Ni, Ti and Al elemental L-absorption edges in the energy loss spectrum. Manual and automated segmentation proce...

متن کامل

Ultrastructure of Plant Leaf Cuticles in relation to Sample Preparation as Observed by Transmission Electron Microscopy

The leaf cuticular ultrastructure of some plant species has been examined by transmission electron microscopy (TEM) in only few studies. Attending to the different cuticle layers and inner structure, plant cuticles have been grouped into six general morphological types. With the aim of critically examining the effect of cuticle isolation and preparation for TEM analysis on cuticular ultrastruct...

متن کامل

Design of a nickel-base superalloy using a neural network

A new computational tool has been developed to model, discover, and optimize new alloys that simultaneously satisfy up to eleven physical criteria. An artificial neural network is trained from pre-existing materials data that enables the prediction of individual material properties both as a function of composition and heat treatment routine, which allows it to optimize the material properties ...

متن کامل

On APFIM of Grain Boundaries in a Nickel Base Superalloy

Experimental details of atom probe field ion microscopy (APFIM) of a Ni-16Cr-9Fe alloy are presented. In particular, studies concerning analysis of intergranular carbides and borides and segregation to grain boundaries are described. It was found that NiZ3B6 precipitates are very sensitive to preferential field evaporation, which necessitates optimization of the analysis conditions. In the FIM ...

متن کامل

Transmission Electron Microscopy in Cell Biology: sample preparation techniques and image information

Transmission electron microscopy is a proven technique in the field of cell biology and a very useful tool in biomedical research. Innovation and improvements in equipment together with the introduction of new technology have allowed us to improve our knowledge of biological tissues, to visualize structures better and both to identify and to locate molecules. Of all the types of microscopy expl...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 32  شماره 6

صفحات  852- 859

تاریخ انتشار 2019-06-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023