RECOVERY OF IRON FROM LOW-GRADE HEMATITE ORE USING COAL-BASED DIRECT REDUCTION FOLLOWED BY MAGNETIC SEPARATION
نویسندگان
چکیده مقاله:
In the present work, iron recovery from a low-grade hematite ore (containing less than 40% iron), which is not applicable in common methods of ironmaking, was studied. Non-coking coal was used as reducing agent. Reduction experiments were performed under various coal to hematite ratios and temperatures. Reduction degree was calculated using the gravimetric method. Reduced samples were subjected to magnetic separation followed by X-ray diffraction analysis. Total iron content, degree of metallization and recovery efficiency in magnetic part were determined by quantitative chemical analysis, which were obtained about 82%, 95% and 64% respectively under optimal conditions. CaO as an additive improved ore reducibility and separation efficiency. The microstructure of reduced samples and final products were analyzed by scanning electron microscopy. Final product with a high degree of metallization can be used in steel making furnaces and charging of blast furnaces which can improve production efficiency and decrease coke usage.
منابع مشابه
Characterization of Sangan low-grade iron ore and its processing by dry low-intensity magnetic separation
In Sangan iron mine nearly two million tons of low-grade iron ore has been extracted and deposited in the mining site and currently no action is made on them. On the other hand, the mining site is located in the semi-arid region and wet processing has been restricted due to water shortage. In this research, the upgradation of Sangan low-grade iron ore from mine B has been performed by dry low-i...
متن کاملBeneficiation of a low-grade iron ore by combination of wet low-intensity magnetic separation and reverse flotation methods
Beneficiation of a low-grade iron ore was investigated by combination of the low-intensity magnetic separation and reverse flotation methods. The main constituents of the representative sample were 36.86% Fe, 8.1% FeO, 14.2% CaO, 13.6% SiO2, and 0.12% S based on the X-ray fluorescence, titration, and Leco analysis methods. The mineralogical studies by the X-ray diffraction, scanning electron mi...
متن کاملThe Layered Reduction of Hematite (Iron Oxide) Ore by Non-Coking Coal: The Effect of Calcium Carbonate on Reduction
Due to the abundance of the non-coking coal and limitations as well as the high costs of the natural gas, the present study examined the direct reduction of hematite (iron oxide) ore in the temperature range of 800-1000 °C by the non-coking coal volatiles. Approximately, 74.9% of the total amounts of volatiles and gases exit the coal up to 800°C. The onset temperature to exit volatiles from the...
متن کاملOptimization of parameters affecting recovery of copper from Sarcheshmeh low-grade sulfide ore using Bioleaching
In this work, the parameters affecting the recovery of copper from the low-grade sulfide minerals of Sarcheshmeh Copper Mine were studied. A low-grade sulfide ore was used with a copper grade of 0.25%, which was about 28% of the mineral oxide, and the sulfide minerals made up the rest. Much more sulfide minerals were found to be pyrite and most of the gangue minerals were quartz, anorthite, bio...
متن کاملUpgrading of High-Aluminum Hematite-Limonite Ore by High Temperature Reduction-Wet Magnetic Separation Process
Abstract: The huge consumption of iron ores in China has attracted much attention to utilizing low grade complex iron resources, such as high-aluminum hematite-limonite ore, which is a refractory resource and difficult to upgrade by traditional physical concentration processes due to the superfine size and close dissemination of iron minerals with gangue minerals. An innovative technology for a...
متن کاملthe layered reduction of hematite (iron oxide) ore by non-coking coal: the effect of calcium carbonate on reduction
due to the abundance of the non-coking coal and limitations as well as the high costs of the natural gas, the presentstudy examined the direct reduction of hematite (iron oxide) ore in the temperature range of 800-1000 °c by thenon-coking coal volatiles. approximately, 74.9% of the total amounts of volatiles and gases exit the coal up to800°c. the onset temperature to exit volatiles from the no...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 13 شماره 3
صفحات 60- 71
تاریخ انتشار 2016-09
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023