Un-doped and Cd-doped ZnZrO3/ZnO/ZrO2 nano composites (CDZZ-NCPs) (CD0-4) were synthesized by the hydrothermal method. The nano composites were characterized by various techniques such as Fourier Transform Infra-Red spectroscopy (FT-IR), X-ray Diffraction (XRD), Field Emission Scanning Electron Microscopy (FE-SEM) and Energy Dispersive X-Ray Analysis (EDS). The photocatalytic properties of CDZZ-NCPs (CD0-4) were studied by degradation of congo red (CR) dye under sunlight irradiation. The results reveal unique sunlight photocatalytic ability for the degradation of CR. The experimental demonstrated that the 0.03 g of ZnZrO3/ZnO/ZrO2 nano composites can degradate 50 mL of CR solution (10 ppm) during 5 minutes (up to 91.3%).

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Photocatalytic degradation of Congo Red dye by using nano ZnO and Ni-Co-ZnO nanocomposites

Photocatalysis has attracted significant attention as a potential issue for the degradation of toxic organic pollutants such as Congo Red. In this research spherical Pure ZnO nano particles and Ni-Co-ZnO nano composites (Zn0.95Ni0.04Co0.01O,  Zn0.95Ni0.025Co0.025O and  Zn0.95Ni0.01Co0.04O) have been synthesized by precipitation method. X- ray diffraction, Fourier transform Infra Red ,field emis...

متن کامل

Sonosynthesis and Characterization of TiO2/ZrO2 Nanocomposite and Photocatalytic degradation of Congo red Dye under UV Light

NanoTiO2 , nanoZrO2 and TiO2 /ZrO2 nanocomposite were prepared via sol gel method by using ultrasonic irradiation. The precursor sol of zirconium was prepared from an aqueous solution of ZrCl4 and titanium tetra 2-propoxide was diluted by 2-propanol and deionized water The TiO2 /ZrO2 nanocomposite was synthesized from directly mixing Titanium dried gel into Zirconium gel. The reaction mixture w...

متن کامل

Preparation of Different WO3 Nanostructures and Comparison of Their Ability for Congo Red Photo Degradation

Tungsten trioxide nanoparticles with monoclinic structure and average particle size about 80 nm were prepared by the spray pyrolysis method. WO3 nanorods with hexagonal structure and average dimension about 15 × 100 nm were synthesized in gram quantities by modified hydrothermal method at lower temperature and shorter reaction time in comparison to the previous research. Photo de...

متن کامل

Photocatalytic degradation of methyl orange and Congo red using C,N,S-tridoped SnO2 nanoparticles

In this study, the photocatalytic degradation of methyl orange and Congo red dye was investigated inaqueous solution using C,N,S-tridoped SnO2 nanoparticles as a nano photocatalyst. The degradationwas carried out under different conditions including the photocatalyst amount, initial concentrationand pH of the solution. The results indicated that the degradation of methyl orange and Congo redwas...

متن کامل

Preparation and characterization of Montmorillonite/ZrO2 nanocomposite and its application for removal of Congo red

Montmorillonite/ZrO2 nanocomposites were prepared by the sol-gel method underultrasonic irradiation. The montmorillonite was incorporated into Zirconium gel. After stirring for 24 hr, the mixture was irradiated for 30 min under ultrasonic irradiation. The filtrated composite gel was calcinated at 400°C for 3h in furnace. The morphology of prepared catalysts was characterized by field emis...

متن کامل

Synthesis and characterization ZnFe2O4@MnO and MnFe2O4@ZnO magnetic nanocomposites: Investigation of photocatalytic activity for the degradation of Congo Red under visible light irradiation

In the present investigation, ZnFe2O4@MnO and MnFe2O4@ZnO magnetic nanocomposites were fabricated via a facile hydrothermal method and were calcined at 300 °C for 3 h. Synthesis of ZnFe2O4@MnO and MnFe2O4@ZnO magnetic nanocomposites optimized by the different weight percentages. The synthesized photocatalyst...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 11  شماره 1

صفحات  32- 40

تاریخ انتشار 2020-01-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023