Oxidation resistance of the nanostructured YSZ coating on the IN-738 superalloy

نویسندگان

  • Ahmad Keyvani Department of Metallurgy and Materials Engineering, Faculty of Technology and Engineering, Shahrekord University, Iran
  • Mohsen Saremi School of Metallurgy and Materials, College of Engineering, University of Tehran, Iran.
چکیده مقاله:

Conventional and nanostructured YSZ coatings were deposited on the IN-738 Ni super alloy by the atmospheric plasma spray technique. The oxidation was measured at 1100°C in an atmospheric electrical furnace. According to the experimental results the nanostructured coatings showed a better oxidation resistance than the conventional ones. The improved oxidation resistance of the nanocoating could be explained by the change in structure to a dense and more packed structure in this coating. The mechanical properties of the coatings were tested using the thermal cyclic, nanoindentation and bond strength tests, during which the nanostructured YSZ coating showed a better performance by structural stability.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

oxidation resistance of the nanostructured ysz coating on the in-738 superalloy

conventional and nanostructured ysz coatings were deposited on the in-738 ni super alloy by the atmospheric plasma spray technique. the oxidation was measured at 1100°c in an atmospheric electrical furnace. according to the experimental results the nanostructured coatings showed a better oxidation resistance than the conventional ones. the improved oxidation resistance of the nanocoating could ...

متن کامل

the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)

cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...

the washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests

در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است

15 صفحه اول

the effect of e-64 on the developmental competence of sheep cocs during in vitro maturation

in the present study, the effect of e-64 at different concentrations (0.5, 1, 5 and 10 µm) added to (1) the ivm medium on oocyte nuclear maturation and developmental competence of ovine oocytes, and (2) to the ivc medium on embryonic development of ovine embryos were investigated.

the effects of changing roughness on the flow structure in the bends

flow in natural river bends is a complex and turbulent phenomenon which affects the scour and sedimentations and causes an irregular bed topography on the bed. for the reason, the flow hydralics and the parameters which affect the flow to be studied and understand. in this study the effect of bed and wall roughness using the software fluent discussed in a sharp 90-degree flume bend with 40.3cm ...

the impact of e-readiness on ec success in public sector in iran the impact of e-readiness on ec success in public sector in iran

acknowledge the importance of e-commerce to their countries and to survival of their businesses and in creating and encouraging an atmosphere for the wide adoption and success of e-commerce in the long term. the investment for implementing e-commerce in the public sector is one of the areas which is focused in government‘s action plan for cross-disciplinary it development and e-readiness in go...

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 47  شماره 2

صفحات  89- 96

تاریخ انتشار 2014-12-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023