Nickel-based Superalloy Layer Deposited on AISI H13 Hot Tool Steel Base Metal Using Explosion Cladding process

نویسندگان

  • A. Amadeh School of Metallurgy and Materials Engineering, Faculty of Engineering, University of Tehran, Tehran, Iran
  • G. Liaghat Faculty of Engineering, Tarbiat Modares University, Tehran, Iran
  • H. Bakhtiari Department of Materials Engineering, Najafabad Branch, Islamic Azad University, Najafabad, Iran
  • M. Khanzadeh Department of Materials Engineering, Science and Research Branch, Islamic Azad University, Tehran, Iran
  • S. A. Akbarimusavi School of Metallurgy and Materials Engineering, Faculty of Engineering, University of Tehran, Tehran, Iran
چکیده مقاله:

An experimental test was carried out to explosively clad solution annealed Inconel 718 superalloy on quench-tempered AISI H13 hot tool steel. A wavy with vortices interface geometry was obtained from this experiment. A gradual change in the wavelength along the direction of welding was observed which was due to a change in the impact angle, following the plate contacts. In this paper, the experiment was simulated by the use of ABAQUS version 6.9 finite element software. The Williamsburg equations of state and Johnson- Cook constitutive equation were used to model the behavior of the explosive and plates, respectively. The numerical result showed that high localized plastic deformation was produced at the bond interface. Pressure magnitude was high enough to create deformation twins and slip lines in the vicinity of Inconel interface to accommodate the plastic deformation caused by shock wave velocity. SEM observation showed that the number of thin melt pockets produced in front of vortices at the interface of Inconel 718 was higher than that of AISI H13 steel. The reason was attributed to the difference between the thermal conductivity of welded alloys. The change of hardness was found to be more severe in superalloy than in steel.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Optimization of process parameters for pulsed laser milling of micro-channels on AISI H13 tool steel

This paper focuses on understanding the influence of laser milling process parameters on the final geometrical and surface quality of micro-channel features fabricated on AISI H13 steel. Optimal selection of process parameters is highly critical for successful material removal and high dimensional and surface quality for micro-sized die/mold applications. A set of designed experiments is carrie...

متن کامل

Hot Forming of Aisi A2 Tool Steel

In order to optimize the hot forming process of tool steels, further improvement of flow stress prediction and additional knowledge on hot deformability, especially at lower and upper limits of the hot working range, are required. The hot working ranges for these steels are very narrow as a consequence of the role of alloying elements, which form carbides. Carbides improve tool steel’s hardenab...

متن کامل

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

Surface integrity predictions and optimisation of machining conditions in the turning of AISI H13 tool steel

Surface integrity (SI) plays a very important role in functional performance. It is dependent on a large number of machining parameters. The major concern of industry is to know which combination of machining parameters provides the best SI of machined components. Traditionally, surface roughness is considered to be the principal parameter to assess the SI of a machined part. However, residual ...

متن کامل

INVESTIGATION NITRIDE LAYERS AND PROPERTIES SURFACES ON PULSED PLASMA NITRIDED HOT WORKING STEEL AISI H13

Nitriding is a surface treatment technique used to introduce nitrogen into metallic materials to improve their surface hardness, mechanical properties, wear resistance and corrosion resistance. In this research, the effects of plasma nitriding parameters including frequency and duty cycle were investigated on samples with different grooves dimensions. Steel blocks prepared from DIN1.2344 hot wo...

متن کامل

Laser deposited TiC/H13 tool steel composite coatings and their erosion resistance

The present work studies the synthesis and performance of TiC/H13 tool steel composite coatings obtained by the laser deposition technique. he effect of laser beam-scanning speeds and the concentrations of TiC in injected powder on the morphologies and microstructures of deposited eads are investigated. The results show that the beam-scanning speeds affect the size and morphology of the beads. ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 14  شماره 2

صفحات  16- 26

تاریخ انتشار 2017-12-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023