Investigation on Process Parameters of Ball Screw Finishing Using Magnetic Abrasive Field
نویسندگان
چکیده مقاله:
Surface finishing is one of the most significant steps in industries which are engaged with surface quality. Finishing by magnetic field is a new method of surface finishing. In this process, machining is executed in mechanical way and semi-homogeneous abrasive slurry performs finishing of surfaces. Needed force to grind surfaces is made by magnetic field. Therefor this method is considered as an advanced machining method. One of application of advanced machining methods is working in situation which conventional methods are not applicable. Nowadays helical and spiral parts have an important position in industry. This result in more attention about manufacturing and finishing of parts. This mechanism is used to finish helical ball screw in CNC machine using magnetic field created by Nd-Fe-B permanent magnet. In executed experiments four parameters which affected on surface quality were investigated. These parameters included feed rate, particles size and amount of ferromagnetic particles. The effect of most parameters was positive and caused to improve surface quality, but generally each parameter had an optimum amount in which by reaching this amount, reducing in efficiency and surface quality was observed. Also, some parameters such as cutting speed had lower effect. The initial specimen had surface roughness of 1.017 µm and the best resultant surface quality was 0.325 µm.
منابع مشابه
effect of the magnetic abrasive finishing (maf) parameters on ball screw finishing process
0
متن کاملInvestigation of the Effective Parameters on Surface Roughness in Magnetic Abrasive Finishing Process Using Design of Experiments
In this article, the effect of parameters like working gap, work piece rotational speed and material removal mechanism(injection of the SiC Abrasive slurry and Al2O3, use of diamond paste as abrasive tool) in Magnetic Abrasive Finishing process using designing of experiments on the external surface of Cylindrical work pieces of Stainless steel AISI 440C to get minimum surf...
متن کاملInvestigation of the Effective Parameters on Surface Roughness in Magnetic Abrasive Finishing Process Using Design of Experiments
In this article, the effect of parameters like working gap, work piece rotational speed and material removal mechanism(injection of the SiC Abrasive slurry and Al2O3, use of diamond paste as abrasive tool) in Magnetic Abrasive Finishing process using designing of experiments on the external surface of Cylindrical work pieces of Stainless steel AISI 440C to get minimum surf...
متن کاملMeasurement and simulation of magnetic field strenght in the nano magnetic abrasive finishing process
Magnetic abrasive finishing can be classified as a non-traditional super finishing method for finishing surfaces with different shapes and working materials like flat plates, shafts, bearings parts, screws, tubes and many other mechanical parts that need good surface finishing properties. MAF is effective in polishing, cleaning, deburring and burnishing metal parts. The most important parameter...
متن کاملinvestigation of the effective parameters on surface roughness in magnetic abrasive finishing process using design of experiments
in this article, the effect of parameters like working gap, work piece rotational speed and material removal mechanism(injection of the sic abrasive slurry and al2o3, use of diamond paste as abrasive tool) in magnetic abrasive finishing process using designing of experiments on the external surface of cylindrical work pieces of stainless steel aisi 440c to get minimum surface roughness has been...
متن کاملMicromachining the Aluminium Tubes Using Abrasive Finishing in Alternating Magnetic Field
This study introduced a method based on magnetic field assisted finishing mechanism for micromachining the inner surfaces of Aluminum tubes. In this approach, using the alternating magnetic field of an AC electromotor, abrasive particles were formed as Magnetic Rods (Magnetic Clusters) and surface micromachining was carried out by the dynamic particular pattern made by an alternating magnetic f...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 7 شماره 3
صفحات 13- 21
تاریخ انتشار 2014-12-22
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023