Investigation of the Effect of Homogenization Treatment on Distribution of Alloying Elements, Microstructure and Hardness of Co-Al-W-Ti-Ta-Base Superalloy

نویسندگان

چکیده مقاله:

The aim of this study was to investigate the effect of temperature and time of homogenization treatment on the microstructure, distribution of alloying elements and hardness of the novel Co-based superalloy Co-7Al-7W-4Ti-2Ta. For this purpose, the specimens were first homogenized at 1250 and 1300 °C for 2, 4, 6 and 8 hours and then water-cooled. Subsequently, the specimens were subjected to hardness testing and microstructural examinations by optical and electron microscopy. The results showed that by increasing the homogenization temperature to 1300 °C, the porosity created by Ti oxidation and local melting of the Co-Al-Ti eutectic compounds led to a decrease in hardness to 90 Vickers. This phenomenon was due to high segregation of alloying elements in the cast structure. The intensity and destructive effects of this segregation were reduced by remelting of alloy. However, by homogenization at 1250 °C, no local melting of eutectic zones or porosity were observed in the specimens and a more uniform structure was obtained with increasing time. Minimum and maximum hardness values after homogenization at 1250°C were 348 and 406 Vickers, respectively. Moreover, the microstructure became more homogenous by increasing the homogenization treatment time at this temperature.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

an investigation of the impact of self monitoring on langauge teachers motivational practice and its effect on learners motivation

the central purpose of this study was to conduct a case study about the role of self monitoring in teacher’s use of motivational strategies. furthermore it focused on how these strategies affected students’ motivational behavior. although many studies have been done to investigate teachers’ motivational strategies use (cheng & d?rnyei, 2007; d?rnyei & csizer, 1998; green, 2001, guilloteaux & d?...

the effect of task complexity on lexical complexity and grammatical accuracy of efl learners’ argumentative writing

بر اساس فرضیه شناخت رابینسون (2001 و 2003 و 2005) و مدل ظرفیت توجه محدود اسکهان (1998)، این تحقیق تاثیر پیچیدگی تکلیف را بر پیچیدگی واژگان و صحت گرامری نوشتار مباحثه ای 60 نفر از دانشجویان زبان انگلیسی بررسی کرد. میزان پیچیدگی تکلیف از طریق فاکتورهای پراکندگی-منابع تعیین شد. همه ی شرکت کنندگان به صورت نیمه تصادفی به یکی از سه گروه: (1) گروه موضوع، (2) گروه موضوع + اندیشه و (3) گروه موضوع + اندی...

15 صفحه اول

the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)

cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...

: the effect of sericin levels (silk glue protein) on rate of in vitro maturation, fertilization and culture of sheep oocytes

هدف از آزمایش اول بررسی اثر سطوح مختلف سریسین [0 (control), 0.1, 0.5, 1.0, 2.5 %] افزوده شده به محیط , ivm بر cumulus cell expansion، بلوغ هسته و توسعه متوالی جنین، در گوسفندان نژاد سنجابی در فصل تولید مثلی می باشد. از سرگیری میوز به وسیله خارج شدن اولین پولار بادی اندازه گیری و هم چنین درصد رسیدن جنین های دو سلولی به مرحله کلیواژ و بلاستوسیت نیز به عنوان نشانه ای از میزان شایستگی توسعه اولیه ج...

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 39  شماره None

صفحات  103- 119

تاریخ انتشار 2020-08

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

کلمات کلیدی برای این مقاله ارائه نشده است

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023