  Objective: Orthodontic wires should have high resistance against corrosion in the oral environment. Since the effect of pH on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva.   Methods: This in vitro experimental study was conducted on 24 mandibular central incisor brackets of 4 manufacturers namely Dentaurum, American Orthodontics, Shinye and ORJ. The brackets were immersed in acidic artificial saliva along with stainless steel (SS) or NiTi 0.016 round wires for 28 days. All specimens were weighed before and after the experiment by a digital scale. After the experiment, the specimens were evaluated under a light stereomicroscope and specimens with corrosion were further assessed by scanning electron microscope (SEM) and energy-dispersive X-ray spectroscopy (EDX). Two-way ANOVA was used for statistical analysis.   Results: The mean corrosion rate (CR) was -1.80, 0.11, 0.05 and -0.93 mpy for Dentaurum, American Orthodontics, Shinye and ORJ brackets, respectively in combination with NiTi wire these values were 0.46, -0.71, 0.87 and -0.27 mpy, respectively in combination with SS wires the differences in this regard were not statistically significant (p>0.05). Micrographs showed high corrosion in ORJ brackets followed by Shinye brackets. EDX showed that the combination of ORJ bracket with SS wire had the highest iron (Fe) content and the highest CR. Conclusion: SS brackets manufactured by Shinye and ORJ companies in combination with SS wires showed higher CR in acidic artificial saliva compared to other bracket/wire combinations.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

galvanic corrosion of orthodontic brackets and wires in acidic artificial saliva: part ii

objective: orthodontic wires should have high resistance against corrosion in the oral environment. since the effect of ph on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva.   methods: this in vitro experimental study was conducted on 24 mandibular central...

متن کامل

Galvanic Corrosion and Ion Release from Different Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part I

  Objective: Corrosion resistance is among the most important properties of metal alloys used in the oral cavity. Consumption of acidic foods reduces the salivary pH and intensifies the corrosion of brackets and orthodontic wires. This study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artifici...

متن کامل

galvanic corrosion and ion release from different orthodontic brackets and wires in acidic artificial saliva: part i

objective: corrosion resistance is among the most important properties of metal alloys used in the oral cavity. consumption of acidic foods reduces the salivary ph and intensifies the corrosion of brackets and orthodontic wires. this study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artificial sali...

متن کامل

Galvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes.

The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested i...

متن کامل

Galvanic Corrosion among Different Combination of Orthodontic Archwires and Stainless Steel Brackets

Introduction: The aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. Methods: Three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. Three groups consisted of different wire-bracket couples and one group ...

متن کامل

Galvanic Corrosion of and Ion Release from Various Orthodontic Brackets and Wires in a Fluoride-containing Mouthwash.

Background and aims. This study compared the galvanic corrosion of orthodontic wires and brackets from various manufacturers following exposure to a fluoride mouthwash. Materials and methods. This study was conducted on 24 lower central incisor 0.022" Roth brackets of four different commercially available brands (Dentaurum, American Orthodontics, ORJ, Shinye). These brackets along with stainles...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 33  شماره None

صفحات  88- 97

تاریخ انتشار 2015-03

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023