Fractographic Aspects of Stress Corrosion Failure of Zircaloy 2 in CH3OH HCL Solutions

نویسنده

چکیده مقاله:

Fracture surface of Zircaloy-2 specimens tested under constant crosshead speed in CH3OH/0.4 Vol. %HCI solution with and without selenium (25 ppm) addition was studied. Using a combined process of deformation and annealing, coarse grained material was also obtained and examined. Two modes of stress corrosion crack propagation were observed: an intergranular zone caused by stress assisted anodic dissolution, and a transgranular cleavage zone, due to hydrogen absorption.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

AN INVESTIGATION ON CORROSION BEHAVIOUR OF A356-10 VOL.% SiC COMPOSITES IN HCl SOLUTIONS

In this study, corrosion behaviour of A356-10 vol.% SiC composites casted by gravity and squeeze casting is evaluated. For this purpose, prepared samples were immersed in HCl solution for 1h at open circuit potential. Tafel polarization and electrochemical impedance spectroscopy (EIS) were carried out to study the corrosion resistance of composites. The Tafel polarization and EIS studies of ...

متن کامل

INHIBITION OF CORROSION OF CARBON STEEL IN HCl SOLUTIONS BY VARIOUS SCHIFF BASE

Evaluation of corrosion inhibitors for steel in acidic media is important for some industrial facilities as well as is very interesting from theoretical aspects. Most of the effective inhibitors are organic compounds containing nitrogen, phosphorus and sulphur in their structures [1, 2]. Heteroatoms such as nitrogen, oxygen and sulphur are capable of forming coordinate covalent bond with metal ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 3  شماره 1

صفحات  23- 30

تاریخ انتشار 1990-05-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023