Background and Aims: Today, resin composites are one of the most commonly used materials in restorative dentistry. However, failure in resin treatments is also common due to its chemical nature and its high talent for decay recurrence. According to conservative approaches, "conservative" treatments are more likely to be considered than "Replacement" of damaged remedies. The purpose of this study was to compare different surface preparation methods on composite surfaces to achieve the highest bond strength between the old and new composites after accelerated aging. Materials and Methods: First, composite cylinders with a diameter of 6 and a height of 5 mm were prepared using an incremental technique and a microhybrid resin composite. The specimens were stored in distilled water for 6 months at 37°C and then the surfaces of all aged compsites were roughened using diamond milling followed by phosphoric acid etching. The specimens were randomly subjected into five groups. Group 1: GC Composite Primer. Group 2: Universal bonding containing silane (Kuraray). Group 3: Self etching adhesive (SE bond; Kuraray) Group 4: silane (Ivoclar Vivadent) + Second bottle of SE bond bonding system (Kuraray). Group 5: control group with no treatment. Then, 5 mm incremental of new composite (similar to the aged composite with different color) were placed on the surfaces of specimens, sectioned, and thermocycled for 3000 cycles for the microtensile bond strength evaluation. The specimens were evaluated using a stereomicroscope after failure. Data were analyzed by one-way ANOVA and Post Hoc Tukey test. Results: The specimens in which silane and SE bond were used showed the highest mean microtensile bond strength and those treated by universal bond showed the least bond strength which were significantly different (P=0.02). All samples had cohesive failure patterns in all groups and the percentage of failures in old and new composites did not differ significantly (P=0.69). Conclusion: : Based on the results, all surface preparations used in this study could provide an appropriate bond strength for repair of old composite restorations. Also, the microtensile bond strength between the old and new composites was higher than the cohesive strength of resin composite itself. However, the mean microtensile bond strength value for the group treated by universal bond was significantly lower than those treated by silane and hydrophobic containing bonding system.
منابع مشابه
Microtensile bond strength of repaired indirect resin composite
PURPOSE The objective of this study was to investigate the effect of surface treatments on microtensile bond strengths (MTBSs) of two types of indirect resin composites bonded to a conventional direct resin composite. MATERIALS AND METHODS Indirect resin composite blocks of Ceramage and SR Nexco were prepared in a plastic mold having a dimension of 10 × 10 × 4 mm. These composite blocks were ...
متن کاملEffect of surface pretreatments on the microtensile bond strength of lithium-disilicate ceramic repaired with composite resin.
The aim of this study was to evaluate the influence of ceramic surface treatments and silane drying temperature on the microtensile bond strength (µTBS) of a resin composite to a lithium disilicate ceramic. Twenty blocks (7x7x5 mm) of lithium disilicate-based hot-pressed ceramic were fabricated and randomly divided into 4 groups: G1: acid etching with 9.5% hydrofluoric acid for 20 s and drying ...
متن کاملA comparative evaluation of shear bond strength of immediately repaired composite resin – An in-vitro study
The aim of this study is to “evaluate the shear bond strength of immediately repaired light cured composite resin using different bonding agents”. Forty recently extracted human incisors were mounted on acrylic resin blocks and cavity (5 × 3mm) was prepared at the middle third of the crown. The prepared cavity was etched, rinsed, dried and restored using Single bond adhesive (3M), composite and...
متن کاملIn Vitro Effects of Different Surface Preparation Techniques on Shear Bond Strength of Direct to Indirect Composite Resin
Objective: Repair of an indirect restoration is usually preferred over its replacement. This study aimed to evaluate the effect of silane in different surface preparation techniques on the bond strength of direct to indirect composite resin. Methods: For this in vitro experimental study, 48 indirect composite cubes were fabricated, divided into 4 groups of 12 and subjected to the following ...
متن کاملBond strength of dental nanocomposites repaired with a bulkfill composite
BACKGROUND The aim of this study was to analyze the bond strength of aged resin based nanocomposites repaired with the same and bulk fill composites. MATERIAL AND METHODS Seventy-two disc shaped resin composites consisted of three different nanocomposite resins (Filtek Ultimate/FU, Herculite XRV Ultra/HXRV, and Reflectys/R) were produced. After storing the samples for 8 weeks in distilled wat...
متن کاملEffect of indirect composite treatment microtensile bond strength of self-adhesive resin cements
BACKGROUND No specific indications about the pre-treatment of indirect composite restorations is provided by the manufacturers of most self-adhesive resin cements. The potential effect of silane treatment to the bond strength of the complete tooth/indirect restoration complex is not available.The aim of this study was to determine the contribution of different surface treatments on microtensile...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 32 شماره 1
صفحات 29- 39
تاریخ انتشار 2019-07
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
کلمات کلیدی برای این مقاله ارائه نشده است
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023