Evaluation of corrosion behaviour on Mn-Cr austenitic steels using 0.1 M HCl solution

نویسندگان

  • B. Izadi Faculty of Engineering, Bu-Ali Sina University, Hamedan, Iran.
  • M. Asadi Asadabad Materials Research School, Nuclear Science and Technology Research Institute, Isfahan, Iran.
چکیده مقاله:

One of the attractive low activation steels is the austenitic Mn-Cr steel from the view point of waste disposal because of few long-lived nuclides. In this paper, three types of Mn-Cr austenitic steels were fabricated by vacuum induction furnace. Then plates with 10 mm thickness were fabricated by hot-rolling. The physical metallurgy of these steels was studied by the corrected Schaeffler diagram, X-ray and electron diffraction patterns. The corrected Schaeffler diagram and X-ray diffraction (XRD) results have shown that the matrix of these steels is a single γ-phase structure. Also, the corrosion behaviour in 0.1M HCl solution was evaluated by open-circuit potential, Tafel polarization, and electrochemical impedance spectroscopy (EIS). The results of Tafel polarization experiments show corrosion current density of all three Cr-Mn steels is in the range of 10-4 A cm-2 which indicates their appropriate resistance in this acidic environment. The Nyquist plots showed that polarization resistance from the first to third Cr-Mn steels decreases. This trend is due to increase in corrosion current density which corresponds to Tafel polarization curves.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

corrosion behaviour investigation of the four cr-mn-(ni-free) austenitic steels in 0.1 m h2so4 solution

in this study, the four cr-mn-(ni-free) austenitic steels were fabricated by vacuum induction furnace. then plates with 10 mm thickness were fabricated by hot-rolling. corrosion behaviour of the four cr-mn steels in 0.1 m h2so4 solution was investigated using by open-circuit potential, potentiodynamic polarization, and electrochemical impedance spectroscopy (eis). the results indicated that the...

متن کامل

PHASE STABILITY AND SEMICONDUCTING BEHAVIOUR OF LOW ACTIVATION AUSTENITIC MN-CR STEELS

Four compositions of austenitic Mn-Cr steels have been developed successfully for in-vessel component materials in power plant industry. The phase stability of these Mn-Cr steels was studied by and X-ray diffraction (XRD) patterns. XRD patterns have shown that the matrix of these Mn-Cr steels is a single γ-phase structure. The potentiodynamic polarisation curves suggested that these fabricated ...

متن کامل

Corrosion Behaviour of High-Mn TWIP Steels with Electroless Ni-P Coating

An attempt has been taken to improve the corrosion resistance of twinning-induced plasticity (TWIP) steels (Fe-25Mn and Fe-25Mn-3Al) by electroless Ni-P coating. Corrosion resistance in 3.5% NaCl and 0.1M H2SO4 solutions was characterized by the potentiodynamic polarization curves and Tafel method calculations. It was found that Ni-P coating improved the corrosion resistance by the factor of 4 ...

متن کامل

Study of the Corrosion Resistance of Type 304L and 316 Austenitic Stainless Steels in Acid Chloride Solution

The corrosion resistance of type 304L and 316 austenitic stainless steels in 2M H2SO4 at 0-1.5%NaCl concentrations was studied through potentiodynamic polarization technique and optical microscopy analysis. The corrosion rate, pitting potential, passivation potential and surface morphology of both steel where significantly altered by the Clion concentration, alloy composition and metallurgical ...

متن کامل

Y Studies on Austenitic Stainless Steels

Abstract--In this investigation, the fracture surfaces of SS 304 and SS 316 austenitic steels were analysed using the X-ray fractography technique. In both cases, a decrease in the austenite content was observed at the fracture surface as a result of deformation induced martensite, indicating a linear relation with Km~ within the stable crack growth region. The presence of this martensite was f...

متن کامل

AN INVESTIGATION ON CORROSION BEHAVIOUR OF A356-10 VOL.% SiC COMPOSITES IN HCl SOLUTIONS

In this study, corrosion behaviour of A356-10 vol.% SiC composites casted by gravity and squeeze casting is evaluated. For this purpose, prepared samples were immersed in HCl solution for 1h at open circuit potential. Tafel polarization and electrochemical impedance spectroscopy (EIS) were carried out to study the corrosion resistance of composites. The Tafel polarization and EIS studies of ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 2  شماره 1

صفحات  55- 63

تاریخ انتشار 2014-02-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023