In this research, the effect of annealing and aging temperature as well as the effect of quenching media on the microstructure, hardness and dry sliding wear behavior of Ti-6Al-4V alloy has been studied. Cylindrical samples with the diameter of 10 mm and the height of 20mm were solutionized at 930˚C and 1060˚C for 600 seconds and then were quenched in the cold water and in the air. The samples were aged at different temperature of 480˚C, 550˚C and 610˚C for 360 s to increase the hardness. Heat treated samples were tested using standard pin-on-disc test machine at the applied loads of 100, 150 and 200 N. Microstructural investigations using scanning electron microscope revealed that for the samples solutionized at 930˚C and quenched in the water, the microstructure is composed of primary α and high volume fraction of martensitic α΄ phase with fine precipitated of β between martensitic lathes. In the case of air cooled samples, transformed β has also been appeared in the vicinity of primary α. For the samples solutionized at 1060˚C and quenched in the water, fully martensitic micro structure with fine β precipitates was observed. For the sample solutionized at 1060˚C and air quenched, plate like α and lamellar grain boundary β were detected. The maximum hardness value relates to the sample solutionized at 1060˚C and quenched in water which is equal to 433 HV. Different wear mechanisms, including oxidative wear, scratch, and delamination occurred at the worn surfaces at different applied loads. For the samples quenched in the water, the oxidative wear mechanism governing at low applied load and oxide debris was observed as separate or compacted particles which formed in the contact between pin and steel counter face detached from the sample. At higher applied loads, delamination and scratch mechanism was also observed and metallic plate like debris was detached from the sample. Mechanically mixed layer (MML) was formed on the surface of the pin at high applied loads and for the samples with low hardness value adhesion marks were also revealed on the steel disc. The minimum weight loss in the wear test is related to the sample quenched from the 1060ºC in the cold water and aged at 550 ºC .
منابع مشابه
Effect of Surface Treatment on Tribological Behavior of Ti-6Al-4V Implant Alloy
Titanium alloys are extensively used in various fields of engineering, medicine, aerospace, marine due to its excellent mechanical properties. Its usage is more pronounced today in the field of biomedical implants due to its superior biocompatibility, corrosive resistance and high strength to weight ratio. It has poor abrasive wear resistance due to high coefficient of friction and low thermal ...
متن کاملInfluence of artificial saliva compositions on tribological characteristics of Ti-6Al-4V implant alloy.
The present paper describes the results of tests on the influence of human saliva and its substitutes on tribological characteristics of implant materials on the example of the Ti-6Al-4V (a-Ti) titanium alloy. The saliva substitutes were prepared on the basis of pyrophosphates and mucins dissolved in saline buffer. The results of the presented tribological tests show that the values of the para...
متن کاملHeat Treatment of Ti-6al-4v Produced by Lasercusing
LaserCUSING® is a selective laser melting (SLM) process that is capable of manufacturing parts by melting powder with heat input from a laser beam. LaserCUSING demonstrates potential for producing the intricate geometries specifically required for biomedical implants and aerospace applications. One main limitation to this form of rapid prototyping is the lack of published studies on the materia...
متن کاملOsteoblastic behavior to zirconium coating on Ti-6Al-4V alloy
PURPOSE The purpose of this study was to assess the surface characteristics and the biocompatibility of zirconium (Zr) coating on Ti-6Al-4V alloy surface by radio frequency (RF) magnetron sputtering method. MATERIALS AND METHODS The zirconium films were developed on Ti-6Al-4V discs using RF magnetron sputtering method. Surface profile, surface composition, surface roughness and surface energy...
متن کاملPrecision Grinding of Titanium (Ti-6Al-4V) Alloy Using Nanolubrication
In this current era of competitive machinery productions, the industries are designed to place more emphasis on the product quality and reduction of cost whilst abiding by the pollution-preventing policy. In attempting to delve into the concerns, the industries are aware that the effectiveness of existing lubrication systems must be improved to achieve power-efficient and pollutionpreventing ma...
متن کاملMicrostructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation
Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 14 شماره 3
صفحات 21- 33
تاریخ انتشار 2017-09
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023