Effect of Particle Size on the Structural and Mechanical Properties of Al–AlN Nanocomposites Fabricated by Mechanical Alloying
نویسندگان
چکیده مقاله:
Nanostructured Al composites with 2.5 wt.% aluminum nitride (AlN) were fabricated by powder metallurgy using mechanically milled aluminum powder mixed in a planetary ball mill with different particle sizes of AlN (50 nm and 1 μm) as reinforcement. After 20 h milling, the powders were die-pressed uniaxially in a steel die and then sintered at 670 °C for 2 h. The morphologies and properties of the obtained powders were determined by scanning electron microscopy and X-ray diffraction analysis. The results have indicated that the crystallite sizes of the composites decreased by increasing the milling time, resulting in sizes of 46 nm and 55 nm for the composites containing large (1 μm) and small (50 nm) AlN particles, respectively. After 20 h of milling, the microhardness of the nanocomposites with AlN particle sizes of 1 μm and 50 nm were 101 and 122, respectively. The flexural strength of the composite containing smaller AlN particles (50 nm) was higher than that of the composite containing larger AlN particles (1 μm). The testing results have indicated that the strength and hardness properties of the composite containing smaller AlN particles are better than those of the composite with larger AlN particles.
منابع مشابه
The Structural and Mechanical Properties of Al-2.5%wt. B4C Met-al Matrix Nano-composite Fabricated by the Mechanical Alloying
In this study, aluminum (Al) matrix reinforced with micro-particles (30 µm) and nano-particles (50 nm) boron carbide (B4C) were used to prepare Al-2.5%wt., B4C nano-composite and micro-composite, respectively, using mechanical alloying method. The mixed powders were mechanically milled at 5, 10, 15 and 20 hrs. The XRD results indicated that the crystallite sizes of both the micro-composite and ...
متن کاملdetermination of some physical and mechanical properties red bean
چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...
15 صفحه اولthe structural and mechanical properties of al-2.5%wt. b4c met-al matrix nano-composite fabricated by the mechanical alloying
in this study, aluminum (al) matrix reinforced with micro-particles (30 µm) and nano-particles (50 nm) boron carbide (b4c) were used to prepare al-2.5%wt., b4c nano-composite and micro-composite, respectively, using mechanical alloying method. the mixed powders were mechanically milled at 5, 10, 15 and 20 hrs. the xrd results indicated that the crystallite sizes of both the micro-composite and ...
متن کاملAZ31/HA-Zeolite Nano Crystalline Biocomposite Fabricated by Mechanical Alloying and Powder Metallurgy: Mechanical Properties
Magnesium and its alloys are light, biodegradable, biocompatible metals that have promising applications as biomaterials. Magnesium is potentially useful for orthopedic and cardiovascular applications. However, the corrosion rate of this metal is so high that its degradation occurs before the end of the healing process. One of the ways to improve the corrosion rate is to compose it’s with cer...
متن کاملmodification of nanoclay for improving the physico-mechanical properties of dental adhesives
هدف اصلی این مطالعه تهیه یک سامانه نوین چسب عاجی دندانی بر پایه نانورس پیوند شده با پلی متاکریلیک اسید، نانورس پیوند شده با پلی اکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی متاکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی اکریلیک اسید و نانورس پیوند شده با کیتوسان اصلاح شده با گلایسیدیل متاکریلات است. پیوند پلی متاکریلیک اسید و پلی اکریلیک اسید بر ری سطح نانورس در حضور و ...
Study of milling effect on particle size and mechanical properties of WC-Co composite
The effect of milling on the particle size and mechanical properties Tungsten Carbide - Cobalt composite were investigated. First, raw materials ratios by mechanical milling for 4 hours at 300 rpm were mixed. The powder in the optimum temperature 1350°C at a rate of temperature rise 50°C / min and shelf life of 4 minutes and the pressure MPa 30 were sintered in SPS. The results indicated nearly...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 2 شماره 2
صفحات 73- 78
تاریخ انتشار 2015-11-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023