Controlled Crystallization of LTA Zeolitic Nanoparticles from a Clear Solution Using Organic Template

نویسندگان

  • Dariush Bastani Faculty of Chemical and Petroleum Engineering, Sharif University of Technology, Tehran, I.R. IRAN
  • Hossein Kazemian Department of Chemical and Biochemical Engineering, Faculty of Engineering, The University of Western Ontario (UWO), London, Ontario, CANADA
  • Nazila Esmaeili Faculty of Chemical and Petroleum Engineering, Sharif University of Technology, Tehran, I.R. IRAN
چکیده مقاله:

LTA Zeolite nanoparticles was successfully synthesized from clear solution under controlled conditions using hydrothermal method using tetramethyl ammonium hydroxide as a structural directing agent. The as-synthesized LTA zeolite particles were characterized by powder X-ray Diffraction (XRD) analysis, Scanning Electron Microscopy (SEM), Fourier Transform InfraRed (FT-IR) spectroscopy, Energy Dispersive X-ray (EDX) analysis  and surface area measuring technique of Brunauer, Emmett and Teller (BET). XRD patterns and FT-IR spectra were ascertained the formation of pure crystalline phase of 4A (i.e. LTA) zeolite. SEM micrograph was shown particles size in the range of 60 -170 nm with uniform morphology. The Si /Al ratio of the as-synthesized zeolite nanoparticles was 1.66 with a BET surface area of 421 m2/g.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

controlled crystallization of lta zeolitic nanoparticles from a clear solution using organic template

lta zeolite nanoparticles was successfully synthesized from clear solution under controlled conditions using hydrothermal method using tetramethyl ammonium hydroxide as a structural directing agent. the as-synthesized lta zeolite particles were characterized by powder x-ray diffraction (xrd) analysis, scanning electron microscopy (sem), fourier transform infrared (ft-ir) spectroscopy, energy di...

متن کامل

Removal of BTX Compounds from Wastewaters Using Template Free MFI Zeolitic Membrane

MFI zeolite membranes were prepared on porous α-alumina substrates, using secondary growth of nano-seeded layers. The resulting membranes were characterized by means of Scanning Electron Microscopy (SEM), X-Ray Diffractometry (XRD), and pervaporation performance tests for separation of Benzene, Toluene and Xylene (BTX) mixture from contaminated water. The morphology, thickness, homogeneity,...

متن کامل

removal of btx compounds from wastewaters using template free mfi zeolitic membrane

mfi zeolite membranes were prepared on porous α-alumina substrates, using secondary growth of nano-seeded layers. the resulting membranes were characterized by means of scanning electron microscopy (sem), x-ray diffractometry (xrd), and pervaporation performance tests for separation of benzene, toluene and xylene (btx) mixture from contaminated water. the morphology, thickness, homogeneity, cry...

متن کامل

Removal of Lead from Aquatic Solution Using Synthesized Iron Nanoparticles

   Due to its ability in chemical oxidation of contaminants, iron nanoparticle is a material of choice to remove lead ions from aquatic solutions. In this study a reduction method in solution phase was applied to synthesize thenanoparticles. Afterwards, the size of the synthesized particles were confirmed by Scanning Electron Microscopy. It is worth noting that th...

متن کامل

Arsenic Removal from Aqueous Solution Using Titanium Dioxide Nanoparticles (Anatase)

Background and Objectives: Groundwater sources, as strategic sources of water supply, are of particular importance for human beings. Arsenic is a toxic and carcinogenic contaminant that has been reported to be widely found in groundwater sources. In recent years, adsorption property of nanoparticles has been used to remove arsenic. The present study was performed with the aim of assessing the a...

متن کامل

Template synthesis of gold nanoparticles with an organic molecular cage.

We report a novel strategy for the controlled synthesis of gold nanoparticles (AuNPs) with narrow size distribution (1.9 ± 0.4 nm) through NP nucleation and growth inside the cavity of a well-defined three-dimensional, shape-persistent organic molecular cage. Our results show that both a well-defined cage structure and pendant thioether groups pointing inside the cavity are essential for the Au...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 30  شماره 2

صفحات  9- 14

تاریخ انتشار 2011-06-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023