[ 1 ] - Compressibility and Foaming behavior of steel slag/waste glass compositesby particle size distribution and foam agents
In present research, the foam glass-ceramic composites fabricated by window glass, steel slag and SiC, CaCO3 foaming agents were investigated by press–sintering method. The optimum sintering temperature was obtained at 1200°C with a 3-minutes holding time and 20°C/min heating rate. The optimum pressure level of 80 MPa for achieving the 70 % of relative density was selected. The effec...
[ 2 ] - Investigation of Glass- Steel Slag Foam Composite Sintering in Presence of SiC
Amorphous steel slag was blended with different concentrations of waste glass (20, 40, 50, 60, 70 wt.%) and SiC to obtain a composite. According to Hot Stage Microscopy images, slag-glass composite contractions started at 1050 ºC. scanning electron microscope micrographs of slag-SiC (foaming agent) composite revealed tunnel-like porosities of 500 to 1000 microns. Gaseous products of carbide dec...
Co-Authors