Vulnerability Assessment of Steel Structures in District 12 of Mashhad City and Prioritizing the Welding Defects Using the Analytic Hierarchy Process

Authors

  • reza orangi civil Engineering, Khavaran Institute of Higher Education
Abstract:

Recently, steel structures have been accounted for a large percentage of the buildings due to their advantages such as higher execution speed and easier construction. In steel structures, welded joints are commonly used and their quality plays a key role in stability of buildings under applied loads. Hence, to increase resiliency of welded steel structures against natural hazards, welded joints quality should be improved. In this article, a statistical study was done on welding defects of different connections in 50 welded steel buildings that were being constructed in district 12 (Mashhad, Iran). The reasons for selecting this district were high rates of construction and high potential of hazards. Actually, initial information about joints importance and weld defects were collected by distributed questionnaires among building designer engineers and weld inspectors. In this paper, we used the Expert Choice software that works according to Analytic Hierarchy Process (AHP) to prioritize weld defects in different connections of the buildings and define management solutions to improve them. The priority results revealed that in the non-rigid connections crater, slag inclusion and spatter are more critical whereas in the rigid connections Lack of Penetration (LoP) and Lack of Fusion (LoF) are more critical than the other welding defects in steel building structures.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

assessment of the efficiency of s.p.g.c refineries using network dea

data envelopment analysis (dea) is a powerful tool for measuring relative efficiency of organizational units referred to as decision making units (dmus). in most cases dmus have network structures with internal linking activities. traditional dea models, however, consider dmus as black boxes with no regard to their linking activities and therefore do not provide decision makers with the reasons...

the effect of the record infancy in crimilly acts of guilties (in karaj city)

چکیده یکی از مهمترین دغدغه های بزرگ جوامع بشری، از دیر باز تا کنون که ذهن پژوهشگران و متخصصان بهداشت روانی و اجتماعی و دولتها رابه خود مشغول داشته، مسأله ی بزهکاری می باشد. شناخت کامل پدیده ی بزهکاری و بزهکار، علل وعوامل سقوط یک انسان، چگونگی درمان وی و درنهایت پیشگیری ازبزهکاری ودریک کلام سالم سازی یک جامعه، رسالت عظیم، انسانی ومقدسی می باشد که با بررسی شخصیت مجرم یعنی[ انسانی که تحت شرای...

15 صفحه اول

the analysis of the role of the speech acts theory in translating and dubbing hollywood films

از محوری ترین اثراتی که یک فیلم سینمایی ایجاد می کند دیالوگ هایی است که هنرپیش گان فیلم میگویند. به زعم یک فیلم ساز, یک شیوه متأثر نمودن مخاطب از اثر منظوره نیروی گفتارهای گوینده, مثل نیروی عاطفی, ترس آور, غم انگیز, هیجان انگیز و غیره, است. این مطالعه به بررسی این مسأله مبادرت کرده است که آیا نیروی فراگفتاری هنرپیش گان به مثابه ی اعمال گفتاری در پنج فیلم هالیوودی در نسخه های دوبله شده باز تولید...

15 صفحه اول

Identification and prioritizing of urban disteressed areas factors by applying the fuzzy analytic hierarchy process (FAHP) in Karaj city

The problems of distressed urban areas are getting worse year after year. Due to limited resources and Amenities of municipal organizations for solving every problem concerning urban distressed textures, it is essential to determine the priorities of each area based on identified factors and criteria. In distressed areas, there are different circumstances and distinctive citizens with their nee...

full text

the survey of the virtual higher education in iran and the ways of its development and improvement

این پژوهش با هدف "بررسی وضعیت موجود آموزش عالی مجازی در ایران و راههای توسعه و ارتقای آن " و با روش توصیفی-تحلیلی و پیمایشی صورت پذیرفته است. بررسی اسنادو مدارک موجود در زمینه آموزش مجازی نشان داد تعداد دانشجویان و مقاطع تحصیلی و رشته محل های دوره های الکترونیکی چندان مطلوب نبوده و از نظر کیفی نیز وضعیت شاخص خدمات آموزشی اساتید و وضعیت شبکه اینترنت در محیط آموزش مجازی نامطلوب است.

the crisis of identity in jhumpa lahiris fiction: interpreter of maladies and the namesake

شکل گیری هویت(identity) مقوله مهمی در ادبیات پراکنده مردم(diasporan literature) می باشد. آثار جومپا لاهیری(jhumpa lahiri) ، نویسنده هندی آمریکایی، در سالهای اخیر تحسین منتقدین را به خود معطوف کرده است. وی در این آثار زندگی مهاجران و تلاش آنان برای پیدا کردن جایگاهشان در یک فرهنگ بیگانه را به تصویر کشیده است. این تجربه همواره با احساساتی نظیر دلتنگی برای گذشته، بیگانگی و دوری همراه است. با این ح...

15 صفحه اول

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 31  issue 6

pages  877- 885

publication date 2018-06-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023