The Inhibition Effect of Polyethylenimine (PEI) on Pitting Corrosion of 304 Austenitic Stainless Steel in 3.5% NaCl Solution

Authors

  • A. Afshar Department of Materials Science and Engineering, Sharif University of Technology, Tehran, Iran
  • M. Kazazi Department of Metallurgical & Materials Engineering, Faculty of Engineering, Malayer University, Malayer, Iran
  • M. Sajjadnejad Department of Mining & Metallurgical Engineering, Amirkabir University of Technology, P.O. Box 15875-4413, Tehran, Iran.
Abstract:

One of the problems in the case of stainless steels is their low corrosion resistance against pitting corrosion in chloride containing environments, thereby leading to severe damage to industries. In this research, the pitting corrosion of 304 austenitic stainless steel was studied in 3.5% NaCl solution at room temperature (25˚C) by performing electrochemical measurements (containing cyclic polarization and electrochemical impedance spectroscopy) and immersion measurements. Moreover, the effect of adding different concentrations of PEI inhibitor with two mean molar masses (2000 and 60,000 g/mol) on pitting corrosion was investigated. Finally, the adsorption behavior of this inhibitor on the alloy surface was investigated by ATR-FT.IR and AFM methods. It was observed that both inhibitors prevented uniform and pitting corrosion successfully, but PEI (60,000 g/mol) had better inhibition efficiency than PEI (2000 g/mol).

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

the inhibition effect of polyethylenimine (pei) on pitting corrosion of 304 austenitic stainless steel in 3.5% nacl solution

one of the problems in the case of stainless steels is their low corrosion resistance against pitting corrosionin chloride containing environments, thereby leading to severe damage to industries. in this research, the pitting corrosion of 304 austenitic stainless steel was studied in 3.5% nacl solution at room temperature (25˚c) by performing electrochemical measurements (containing cyclic pola...

full text

IMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE

Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...

full text

Inhibition Effect of 2,2’-bipyridyl on the Corrosion of Austenitic Stainless Steel in 0.5M H2SO4

The corrosion inhibition of AISI309 austenitic stainless steel by 2,2'-Bipyridyl in 0.5M H 2 SO 4 at 298K was studied using the mass loss’ method, the potentiodynamic polarization (Tafel), the linear polarization (LRP) and the electrochemical impedance spectroscopy (EIS). The results showed a mixed inhibition mode and an increase in the charge transfer resistance, due to inhibitor molecules’ ad...

full text

Effect of Crystallographic Orientation on the Pitting Corrosion Resistance of Laser Surface Melted AISI 304L Austenitic Stainless Steel

The localized corrosion behavior of laser surface melted 304L austenitic stainless steel was studied by potentiodynamic polarization test. The extent of improvement in corrosion resistance was governed by the preferred orientation and the percentage of delta ferrite present on the surface of the laser melted sample. It was established by orientation imaging microscopy that the highest pitting p...

full text

Grain Size Effect on the Hot Deformation Processing Map of AISI 304 Austenitic Stainless Steel

In this study, the hot deformation processing map of AISI 304 austenitic stainless steel in two initial grain sizes of 15 and 40 μm was investigated. For this purpose, cylindrical samples were used in the hot compression test at the temperature range of 950-1100 °C and the strain rate of 0.005-0.5% s-1. At first, the relationship between the peak stress and Zener-Hollomon parameter w...

full text

Effect of nitriding temperature on the nanostructure and corrosion properties of Nickel coated 304 stainless steel

Nickel films of 150 nm thickness were deposited on 304 stainless steel and post annealed under flow of nitrogen at different temperatures. The prepared samples were corrosion tested in 1.0 M H2SO4 solution using potentiodynamic polarization technique. Crystallographic and morphological structure of the samples were analysed by X-ray diffraction XRD and atomic force microscopy AFM respectively b...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 10  issue 1

pages  14- 22

publication date 2013-07-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com