In this work, mechanical alloying was employed to produce Ti-50Al and Ti-45Al-5Cr (at%) alloys. Alloying was performed in a planetary mill and the alloying time varying from 5 to 70h. Characterization of the powder mixture was performed by X-ray diffraction (XRD), SEM analyses and DTA test, during mechanical alloying and after annealing at 1100°c in vacuum oven. The results showed, after 50h of milling of TiAl powder mixture, only a complete amorphous phase was detected but with Cr addition (5at%) the Cr (Ti,Al) solid solution within the amorphous matrix were identified. After annealed of mechanically alloyed Ti-50Al for 50h, the γ-phase with high purity and nanostructured size was produced but for sample with Cr addition, TiAl(γ) and amount of Ti3Al(alpha2) were detected. Cr accelerated the production of duplex structure (gamma+alpha2). It suggested the Cr(Ti,Al) solid solution was dissolved in TiAl(gamma) and Ti3Al(alpha2).
similar resources
The Effect of Impurity of Inert Atmosphere on Synthesis of Nanostructure TiAl (γ) Alloy by Mechanical Alloying Process
In this research, the high-energy planetary mill was employed to produce nanocrystalline Ti-50Al(γ)(at%) powders. Initial powders were mechanically alloyed in 99.9999% and 90% purities of Argon and also Air atmosphere with alloying times up to 50h. The effect of impurity of Argon atmosphere on the microstructure and the rate of phase transformation of Ti-50Al were investigated during mechanical...
full textStudying the Effect of Productive Factors on Synthesis of Anostructure Tial (Γ) Alloy By Mechanical Alloying
In this research, the Planetary mill was used for mechanical alloying (MA) of Ti and Alpowder mixture with equal at% (Ti50Al50). The effect of various factors, such as process control agent(PCA), speed of rotation of vial and ball-to-powder weight ratio, on process were studied and the bestcondition to synthesis the alloy was determined. Study on X-ray diffraction (XRD) patterns showedthat at p...
full textA Comparison between the Effect of Cr and W Addition on Formation Kinetic of Nanostructure TiAl(γ) Alloy by Mechanical Alloying Route
In this research, mechanical alloying was used to produce Ti-50Al, Ti-45Al-5Cr and Ti-45Al-5W (at%) alloys. The effect of ternary addition (Cr and W) on microstructure and production efficiency of TiAl alloy were investigated. Alloying was performed in a planetary mill and the milling time varying from 5 to 70h. The structural evaluation in these powders was done by X-ray diffraction (XRD) tech...
full texta comparison between the effect of cr and w addition on formation kinetic of nanostructure tial(γ) alloy by mechanical alloying route
in this research, mechanical alloying was used to produce ti-50al, ti-45al-5cr and ti-45al-5w (at%) alloys. the effect of ternary addition (cr and w) on microstructure and production efficiency of tial alloy were investigated. alloying was performed in a planetary mill and the milling time varying from 5 to 70h. the structural evaluation in these powders was done by x-ray diffraction (xrd) tech...
full textthe effect of impurity of inert atmosphere on synthesis of nanostructure tial (γ) alloy by mechanical alloying process
in this research, the high-energy planetary mill was employed to produce nanocrystalline ti-50al(γ)(at%) powders. initial powders were mechanically alloyed in 99.9999% and 90% purities of argon and also air atmosphere with alloying times up to 50h. the effect of impurity of argon atmosphere on the microstructure and the rate of phase transformation of ti-50al were investigated during mechanical...
full textMy Resources
Journal title
volume 24 issue 2
pages 123- 130
publication date 2011-06-01
By following a journal you will be notified via email when a new issue of this journal is published.
Hosted on Doprax cloud platform doprax.com
copyright © 2015-2023