Surveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by Differential Scanning Calorimetry (DSC)

Authors

  • A. Hassanzadeh Chemistry Department, Urmia University, Urmia, Iran.
  • B. Shaabani Chemistry Department, Tabriz ,University, Tabriz, Iran.
  • E. Hobbolahi Chemistry Department, Islamic Azad University-Ardabil Branch, Ardabil, Iran.
  • M. Alem Chemistry Department, Islamic Azad University-Ardabil Branch, Ardabil, Iran.
  • S. Hedayati Chemistry Department, Islamic Azad University-Ardabil Branch, Ardabil, Iran.
Abstract:

One of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. In this paper, the authors have studied thermal behaviour for Schiff base ligand and their synthesized Cobalt, Nickel complexes. In this method, the sample is opposed to a controlled temperature change and its physical properties. Here we studied melting point and Tg and thermal destructive by surveying DSC thermograms of above compounds. Our team also have surveyed thermograms from the mix of these compounds with nano silver.

similar resources

surveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by differential scanning calorimetry (dsc)

one of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. in this paper, the authors have studied thermal behaviour for schiff base ligand and their synthesized cobalt, nickel complexes. in this method, the sample is opposed to a controlled temperature change and its physical properties. here we studied melting point and tg...

full text

control of the optical properties of nanoparticles by laser fields

در این پایان نامه، درهمتنیدگی بین یک سیستم نقطه کوانتومی دوگانه(مولکول نقطه کوانتومی) و میدان مورد مطالعه قرار گرفته است. از آنتروپی ون نیومن به عنوان ابزاری برای بررسی درهمتنیدگی بین اتم و میدان استفاده شده و تاثیر پارامترهای مختلف، نظیر تونل زنی(که توسط تغییر ولتاژ ایجاد می شود)، شدت میدان و نسبت دو گسیل خودبخودی بر رفتار درجه درهمتنیدگی سیستم بررسی شده اشت.با تغییر هر یک از این پارامترها، در...

15 صفحه اول

Determination of the activation energy of crystallization based up on Ozawa and Kissinger formalisms and thermal stability of V2O5-NiO- TeO2 glasses by differential scanning calorimetry (DSC)

In the present research work, (60-x)V2O5-xNiO-40TeO2 amorphous bulk compositions with different molar percentages of 0≤x≤20 mol%, were prepared by well-known  rapid melt-quenching method. Differential scanning calorimetry (DSC) at different heating rates (φ) was used to thermal analyze and to obtain more insight in to the thermal stability, glass forming tendency and so calorimetric characteris...

full text

Practical Food Applications of Differential Scanning Calorimetry (DSC)

This note describes a number of important food applications utilising the PerkinElmer DSC demonstrating the versatility of the technique as a tool in the food industry.

full text

the effects of error correction methods on pronunciation accuracy

هدف از انجام این تحقیق مشخص کردن موثرترین متد اصلاح خطا بر روی دقت آهنگ و تاکید تلفظ کلمه در زبان انگلیسی بود. این تحقیق با پیاده کردن چهار متد ارائه اصلاح خطا در چهار گروه، سه گروه آزمایشی و یک گروه تحت کنترل، انجام شد که گروه های فوق الذکر شامل دانشجویان سطح بالای متوسط کتاب اول passages بودند. گروه اول شامل 15، دوم 14، سوم 15 و آخرین 16 دانشجو بودند. دوره مربوطه به مدت 10 هفته ادامه یافت و د...

15 صفحه اول

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 1  issue 4

pages  269- 273

publication date 2011-06-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023