Study of Pitting Corrosion Inhibition of Mild Steel by Nitrite in Concrete Pore Solution by Polarization and Zero Resistance Ammetery (ZRA) Techniques (RESEARCH NOTE)

Authors

Abstract:

A research on the corrosion inhibition of mild steel pitting corrosion in concrete pore solution by sodium nitrite was carried out by employing potentiodynamic, potentiostatic polarization and zero resistance ammetery (ZRA) techniques. Passivity breakdown potential was decreased from the transpassive potential of 700 mV at the absence of chloride to a value of -50 mV when just 0.01M NaCl was added to the test solution and further a decrease to -350 mV was recorded when the concentration of chloride was increased to 0.5M. Addition of NaNO2 into the saturated Ca(OH)2 solution containing 0.5M NaCl considerably shifted the pitting potential towards noble values. Similar results of inhibitive effect of nitrite were obtained from couple potential and current measurement between two nominal identical electrodes through ZRA establishment. In the test solution containing NaNO2, continuous increasing of the corrosion potential towards noble values and simultaneous decrease in couple current density towards zero proved the stability and improvement of the passive film. Whereas, continuous decrease in couple potential accompanied with sharp increase in couple current density with a stable value of 3µA/cm2 at the absence of NaNO2 demonstrated the occurrence of pitting corrosion.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

SYNERGISTIC INFLUENCE OF NITRITE ON INHIBITION OF MILD STEEL CORROSION IN CHLORIDE CONTAMINATED ALKALINE SOLUTION

Corrosion behavior of mild steel in chloride contaminated alkaline solution has been studied for the period up to 100days. Saturated Calcium hydroxide solution was used as alkaline solution and 0.5M NaCl solution was used to accelerate mild steel corrosion. The Charge transfer resistance Rct, Current density Icorr and inhibition efficiency values were obtained from tafel polarization and electr...

full text

Corrosion Inhibition of Mild Steel in Acidic Solution by Apricot Gum as a Green Inhibitor

The inhibitive effect of apricot gum AG on mild steel in 0.5 M phosphoric acid solution was investigated by potentiodynamic polarization, electrochemical impedance spectroscopy EIS, linear polarization resistance and electrochemical noise EN techniques. The inhibition efficiency increased with increasing AG concentration up to a certain value and decreased with increasing temperature. Polarizat...

full text

Inhibition of Mild Steel Corrosion in Sulfuric Acid Solution by 2-Hydropyrimidine-2-Thione Derivative

The corrosion inhibition potential and efficacy of 2-hydropyrimidine-2-thione derivative on mildsteel in 0.5 M sulfuric acid solution was investigated using electrochemical polarization and FTIRspectroscopic techniques. In addition, docking studies were carried out as theoretical investigationof adsorption inhibitor on iron surface. The results of polarization studies indicate...

full text

a genre analytic study of research papers written by bilingual writers and their beliefs: a case of persian-english writers

تحقیق حاضر گزارشی است از تحلیل بخش مقدمه دو دسته از مقالات که عبارتند از: 11 مقاله از دو نویسنده دوزبانه فارسی زبان, که شامل مقدمه 4 مقاله به زبان انگلیسی و چاپ شده در مجلات بین المللی, مقدمه 3 مقاله به زبان انگلیسی و 4 مقاله به زبان فارسی چاپ شده در مجلات داخلی می شود؛ و 12 مقاله از محققان خارجی که در مجله applied linguistics به چاپ رسیده است. مبنای تئوری این تحلیل ها نظریه سوئلز (1990) یا هما...

15 صفحه اول

study of cohesive devices in the textbook of english for the students of apsychology by rastegarpour

this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...

Pitting Corrosion Behaviour of New Corrosion-Resistant Reinforcement Bars in Chloride-Containing Concrete Pore Solution

In this study, the pitting behaviour of a new corrosion-resistant alloy steel (CR) is compared to that of low-carbon steel (LC) in a simulated concrete pore solution with a chloride concentration of 5 mol/L. The electrochemical behaviour of the bars was characterised using linear polarisation resistance (LPR) and electrochemical impedance spectroscopy (EIS). The pitting profiles were detected b...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 22  issue 4

pages  369- 380

publication date 2009-12-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023