Microtensile bond strength of clearfil SE bond to caries-affected dentin and normal dentin Dr. A. Ghasemi* - Dr. M. Bargrizan** - Dr. M. Mahmoodi*** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. **- Assistant Professor of Pedodontics Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. ***- Dentist. Background and Aim: Bonding systems have been traditionally used on normal dentin, even though caries-affected and sclerotic dentin are often the clinically relevant bonding substrates. A self-etching primer adhesive system (Clearfil SE Bond) was evaluated for its ability to bond to caries-affected and normal dentin. Materials and Methods: In this experimental study, twelve extracted human primary molars with occlusal caries were selected. The enamel and superficial dentin were ground with a diamond disk and stained with a caries detector solution (propylen glycol and 1% acid red). The red-stained soft dentin which was classified as infected dentin was excavated and the affected dentin and surrounding normal dentin were polished with a 600 grit silicon carbide paper under running water to achieve a flat surface. The entire flat surface was bonded with Clearfil SE Bond (Kuraray) according to the manufacturer’s instructions and covered with composite resin Clearfil AP-X (Kuraray) to form a composite crown, approximately 4.5 mm high. The teeth were stored in distilled water at room temprature for 24 hours and were then sectioned with a diamond saw under running water in both X and Y directions, perpendicular to the bonded surface with dimensions of approximately 0.8-1 mm, so that the bonded areas of the affected or normal dentin were isolated. The obtained rods were divided into two groups: Affected and sound dentin. After measuring the cross-sectional areas at the interface, the specimens were mounted in a microtensile tester machine and pulled under tension to failure. The mode of failure was evaluated using a streomicroscope and the data were analyzed by t-test. Results: Statistical analysis indicated that the microtensile bond strength in affected dentin (21.53±6.52 MPa) was significantly lower (p<0.05) than normal dentin (26.98±7.31 MPa). Conclusion: The studied self-etch system, attained lower microtensile bond strength in affected dentin as compared to normal dentin. Key words: Microtensile - Normal dentin – Affected dentin - Primary teeth
similar resources
Elemental distributions and microtensile bond strength of the adhesive interface to normal and caries-affected dentin.
The aim of this study was to evaluate the microtensile bond strength (microTBS) and the elemental contents of the adhesive interface created to normal versus caries-affected dentin. Extracted human molars with coronal carious lesions were used in this study. A self-etching primer/adhesive system (Clearfil Protect Bond) was applied to flat dentin surfaces with normal and caries-affected dentin a...
full textShear bond strength of different adhesive systems to normal and caries-affected dentin
BACKGROUND AND AIM: According to the effect of the adhesive and substrate type on the bond strength, examination of the adhesive is required in all aspects. The aim of this study was to evaluate the shear bond strength of different adhesive systems to normal dentin (ND) and caries affected dentin (CAD) in permanent teeth. METHODS: Thirty extracted molars with small occlusal caries were selected...
full textThe Effect of Temperature on Shear Bond Strength of Clearfil SE Bond and Adper Single Bond Adhesive Systems to Dentin
STATEMENT OF THE PROBLEM Monomer viscosity and solvent evaporation can be affected by the adhesive system temperature. Higher temperature can elevate the vapor pressure in solution and penetration of adhesive in smear layer. Bonding mechanism may be influenced by the adhesive temperature. PURPOSE This study aimed to evaluate the effect of pre-heating on shear bond strength of etch-and-rinse a...
full textMicrotensile Bond Strength of Self-etching Adhesives to Dentin
The aim of this study was to determine microtensile bond strength of two and one-step self-etching adhesive systems to dentin. 25 intact human third molars were used. Flat surfaces of mid-coronal dentin were exposed and the teeth were divided into 5 groups (n=5). Composite build-ups were made using the following self-etching systems / composite materials: 2-step self-etching system Contax / Ecu...
full textMicrotensile bond strength of bulk-fill restorative composites to dentin
BACKGROUND To facilitate the easier placement of direct resin composite in deeper cavities, bulk fill composites have been introduced. The Mechanical stability of fillings in stress bearing areas restored with bulk-fill resin composites is still open to question, since long term clinical studies are not available so far. Thus, the objective of the study was to evaluate and compare the microtens...
full textthe effect of temperature on shear bond strength of clearfil se bond and adper single bond adhesive systems to dentin
statement of the problem: monomer viscosity and solvent evaporation can be affected by the adhesive system temperature. higher temperature can elevate the vapor pressure in solution and penetration of adhesive in smear layer. bonding mechanism may be influenced by the adhesive temperature. purpose: this study aimed to evaluate the effect of pre-heating on shear bond strength of etch-and-rinse a...
full textMy Resources
Journal title
volume 18 issue 2
pages 8- 14
publication date 2006-05
By following a journal you will be notified via email when a new issue of this journal is published.
No Keywords
Hosted on Doprax cloud platform doprax.com
copyright © 2015-2023