Evaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718

Authors

  • Behrooz Movahedi Assistant Professor, Department of Nanotechnology Engineering, Faculty of Advanced Sciences and Technology, University of Isfahan.
  • Iraj Lirabi Ph.D. Student, Department of Mechanical Engineering, University of Birjand
  • Mehdi Bazargan Lecturer, Islamic Azad University, Khomeinishahr Branch
  • Rasool Mokhtari Homami M.Sc., Department of Mechanical Engineering, Isfahan University of Technology
Abstract:

In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machining of superalloy Inconel 718 in wet and dry conditions indicated that the nanocrystalline coatings could produce better performance of tools in turning. Abrasion and adhesive wear resistance improved by nanocrystalline and modified Aluminum composition in TiAlN coating as well as toughness and thermal stability.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

Investigation of Cutting Forces Superalloy Inconel 718

Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...

full text

Characterization of strain induced precipitation in Inconel 718 superalloy

Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...

full text

Effect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Pressed Superalloy Inconel 718

Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...

full text

the effects of planning on accuracy and complexity of iranian efl students’ written narrative task performance

this study compared the different effects of form-focused guided planning vs. meaning-focused guided planning on iranian pre-intermediate students’ task performance. the study lasted for three weeks and concentrated on eight english structures. forty five pre-intermediate iranian students were randomly assigned to three groups of guided planning focus-on-form group (gpfg), guided planning focus...

15 صفحه اول

Metallurgical Factors Influencing the Machinability of Inconel 718 John J. Schirra, Pratt & Whitney

Because of the large volume of Inconel 718 used by the aerospace and power generation industries and the high percentage of metal removed to machine complex component geometries; understanding and improving the machining characteristics of Inconel 718 would result in substantial cost savings. While progress has been made in developing improved tool materials and machining processes, a detailed ...

full text

the effects of time planning and task complexity on accuracy of narrative task performance

هدف اصلی این تحقیق بررسی تاثیر برنامه ریزی زمانی، هم چنین افزایش میزان پیچیدگی تکالیف در نظر گرفته شده بصورت همزمان، بر دقت و صحت و پیچیدگی عملکرد نوشتاری زبان آموزان می باشد. بدین منظور، 50 نفر از دانش آموزان دختر در رده ی سنی 16 الی 18 سال به عنوان شرکت کنندگان در این زمینه ی تحقیق در نظر گرفته شدند و به دو گروه آزمایشی و کنترل بصورت اتفاقی تقسیم شدند. اعضای گروه آزمایشی هر دو تکلیف ساده و پی...

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 3  issue 2

pages  69- 75

publication date 2010-12-22