Effect of Er:YAG Laser Irradiation on Shear Bond Strength of Two Porcelain Laminate Veneers Bonded to Tooth Surface

Authors

  • Ehsan Morshedi Postgraduate Student, Faculty of Dentistry, Shahed University, Tehran, Iran
  • Maryam Azimi Zavaree Assistant Professor, Department of Prosthodontics, Faculty of Dentistry, Shahed University, Tehran, Iran
  • Maryam Pirmoradian PhD. Candidate, Department of Dental Biomaterials, School of Dentistry, Research Center for Science and Technology in Medicine, Tehran University of Medical Sciences, Tehran, Iran
  • Sara Torabi Periodontist, Tehran, Iran
  • Sayed Shojaedin Shayegh Associate Professor, Department of Prosthodontics, Faculty of Dentistry, Shahed University, Tehran, Iran
  • Seyed Mohammad Reza Hakimaneh Assistant Professor, Department of Prosthodontics, Faculty of Dentistry, Shahed University, Tehran, Iran
  • Sina Jafari Postgraduate Student, Faculty of Dentistry, Shahed University, Tehran, Iran
Abstract:

Background and Aim: The conventional procedure for removal of porcelain laminate veneers (PLVs) is time-consuming and inconvenient. The purpose of this study was to evaluate the efficacy of Er:YAG laser for debonding of PLVs. Materials and Methods: Forty-eight intact extracted human maxillary anterior teeth received discoid PLVs (24 feldspathic and 24 e-max ceramic). The PLVs had 0.7 mm thickness and 4 mm diameter. After cementation of all PLVs with a light-cure cement, samples were stored at 37ºC distilled water for 48 h. Samples of each ceramic were randomly divided into 3 groups of 8 samples. Then, laser was irra-diated on the cemented PLVs as follows: (I) feldspathic PLVs without laser irradiation (control group), (II) feldspathic PLVs with laser irradiation (6 s, 10 Hz, 200 mJ, 2 W), (III) feldspathic PLVs with laser irradiation (6 s, 10 Hz, 300 mJ, 3 W), (IV) e-max PLVs without laser irradiation (control group), (V) e-max PLVs with laser radiation (6 s, 10 Hz, 200 mJ, 2 W), (VI) e-max PLVs with laser irradiation (6 s, 10 Hz, 300 mJ, 3 W). The shear bond strength of all samples was measured using a universal testing machine. We used Mann-Whitney and Kruskal-Wallis tests for data analysis (P<0.05). Results: Laser irradiation decreased the shear bond strength of both ceramics. But this decrease was only significant for the e-max group (P<0.05). No significant difference was found between different laser irradiation powers in the two ceramic groups. Conclusion: Er: YAG laser is effective for debonding of e-max PLVs.

Upgrade to premium to download articles

Sign up to access the full text

Already have an account?login

similar resources

Effect of Provisional Cements on Shear Bond Strength of Porcelain Laminate Veneers

OBJECTIVES The purpose of this study was to evaluate the effect of three provisional cements and two cleaning techniques on the final bond strength of porcelain laminate veneers. METHODS The occlusal third of the crowns of forty molar teeth were sectioned and embedded in autopolymerizing acrylic resin. Dentin surfaces were polished and specimens were randomly divided into four groups (n=10). ...

full text

Comparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain

Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...

full text

Effect of Silane on Shear Bond Strength of Two Porcelain Repair Systems

Objectives: Ceramics have advantages such as optimal esthetics and biocompatibility. However, in the oral environment, they are subjected to high levels of stress due to masticatory forces, saliva, thermal changes and alterations of pH, which increase their risk of fracture. Since replacement of these restorations is costly and time-consuming, composite resin is often used for intraoral repair ...

full text

The effect of surface treatment methods of tooth colored Restorations on shear bond strength

Introduction: Due to undeniable effect of surface treatment on restoration bond strength, this study was conducted to measure and compare the shear bond strength of hybrid ionomer and compomer using the three different methods of surface conditioning. Methods: In this in vitro experimental study, 72 samples were prepared from hybrid ionomer (Vitremer-3M) and compomer (Compoglass-Vivadent) re...

full text

Effect of Er:YAG laser on debonding strength of laminate veneers

OBJECTIVE The purpose of this study was to evaluate the debonding strength of laminate veneers after using erbium-doped: yttrium aluminium garnet (Er:YAG) laser. MATERIALS AND METHODS A total of 60 bovine mandibular incisor teeth were divided into two groups (n = 30). Cylindrical specimens (0.7 mm × 5 mm) were fabricated from Empress II ceramic. Then, they were cemented to incisors using dual...

full text

Bond strengths of porcelain laminate veneers to tooth surfaces prepared with acid and Er,Cr:YSGG laser etching.

STATEMENT OF PROBLEM The erbium, chromium: yttrium, scandium, gallium, garnet (Er,Cr:YSGG) hydrokinetic laser system has been successful in the ablation of dental tissues. It has been reported that this system is also useful for preparing tooth surfaces for adhesion, but results to date have been controversial. PURPOSE This in vitro study evaluated the bond strengths of porcelain laminate ven...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 32  issue 1

pages  21- 29

publication date 2020-01

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023