Development of a new creep testing equipment to obtain long-term deformation parameters of salt rocks

Authors

  • F Sereshki Associate professor, shahrood university of technology
Abstract:

Creep phenomenon in rock engineering plays a key role in development of underground spaces as they must be stable enough for a long period of time. Current research involved designing and manufacturing of a new creep testing machine. The equipment is capable to perform simultaneous light-duty creep tests on more than one cylindrical rock samples at a very low cost.To evaluate the equipment’s performance, a series of creep test was performed on salt rock samples and their axial and lateral deformations were measured by dial gauges. Measurements were taken under constant temperature, humidity and sustained loads. The results revealed that the creep rate in lateral direction was far greater than in the axial direction. Another important conclusion was that both axial and lateral creep curves follow the same pattern with an idealized salt rock creep curve. Also, experiments indicated that the steady state creep rate increases with increasing initial stress state. Also, initial stress state showed a great influence on salt primary creep response.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

development of a new creep testing equipment to obtain long-term deformation parameters of salt rocks

creep phenomenon in rock engineering plays a key role in development of underground spaces as they must be stable enough for a long period of time. current research involved designing and manufacturing of a new creep testing machine. the equipment is capable to perform simultaneous light-duty creep tests on more than one cylindrical rock samples at a very low cost.to evaluate the equipment’s pe...

full text

Prediction of long-term slake durability of clay-bearing rocks

A research program was conducted on different clay-bearing rocks selected from the Ilam, Sarpol-e Zahab and Tajarak regions (Iran) to predict their slaking characteristics. The new durability apparatus (nested mesh drums) separates disintegrated particles varying from > 25.4 to < 2 mm as the drums were rotated. On the basis of the particle size distribution, the disintegration ratio (DR) was us...

full text

the effects of keyword and context methods on pronunciation and receptive/ productive vocabulary of low-intermediate iranian efl learners: short-term and long-term memory in focus

از گذشته تا کنون، تحقیقات بسیاری صورت گرفته است که همگی به گونه ای بر مثمر ثمر بودن استفاده از استراتژی های یادگیری لغت در یک زبان بیگانه اذعان داشته اند. این تحقیق به بررسی تاثیر دو روش مختلف آموزش واژگان انگلیسی (کلیدی و بافتی) بر تلفظ و دانش لغوی فراگیران ایرانی زیر متوسط زبان انگلیسی و بر ماندگاری آن در حافظه می پردازد. به این منظور، تعداد شصت نفر از زبان آموزان ایرانی هشت تا چهارده ساله با...

15 صفحه اول

from linguistics to literature: a linguistic approach to the study of linguistic deviations in the turkish divan of shahriar

chapter i provides an overview of structural linguistics and touches upon the saussurean dichotomies with the final goal of exploring their relevance to the stylistic studies of literature. to provide evidence for the singificance of the study, chapter ii deals with the controversial issue of linguistics and literature, and presents opposing views which, at the same time, have been central to t...

15 صفحه اول

Investigation of Geotextile Yarn Effects on Improvement of Long-Term Deformation of Sandy Soil

Accurate predictions of the amount and the rate of long- term deformation of reinforced soils under an applied load are important key issue in geotechnical engineering, in which the deformation of soil develops with time at a state of constant effective stress. Since geosynthetic is generally considered creep sensitive therefore, evaluation of creep behavior of geosynthetic reinforced soil (GRS...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 3  issue 1

pages  27- 32

publication date 2012-06-05

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023