Determining the Hot Deformation Temperature Range of Medium Carbon Ni-Cr-Mo Low Alloy Steels using Hot Tensile and Hot Torsion Tests

Authors

  • Badri , H. Faculty of Material and Manufacturing Technologies, Malek Ashtar University of Technology, Tehran, Iran.
  • Morakabati, M. Faculty of Material and Manufacturing Technologies, Malek Ashtar University of Technology, Tehran, Iran.
  • Mostafaee Heydarloo, F. Faculty of Material and Manufacturing Technologies, Malek Ashtar University of Technology, Tehran, Iran.
Abstract:

The aim of this study was to investigate the suitable temperature range for hot deformation of three medium carbon Ni-Cr-Mo low alloy steels by hot tensile and hot torsion tests. Hot tensile tests were carried out in the te,prature range of 850-1150°C at a constant strain rate of 0.1 s-1 until fracture. Then, the tensile flow behavior, hot ductility and microstructural evolution of the steels were studied. Hot torsion tests were performed in the temperature range of 1200-780°C at strain of 0.1 with strain rate of 1s-1. The effect of titanium and niobium on the mean flow stress and the non-recrystallization temperature were investigated. The tensile test results showed that dynamic recrystallization was the dominant mechanism at temperatures above 950°C in the base steel and temperatures above 1050°C in the microalloyed steels. The results of hot torsion tests showed that the non-recrystallization temperatures of the base, Ti containing and Nb containing steels were 1070°C, 1069°C and 1116°C, respectively. Finally, the suitable hot deformation temperature range to achieve optimum mechanical properties in the base and Ti containing steels obtained as 950-1070°C and that of Nb containing steel obtained as 950-1100°C.   

Upgrade to premium to download articles

Sign up to access the full text

Already have an account?login

similar resources

Hot Deformation Behavior of Haynes 25 by the Hot Tensile Test

In the present work, hot tensile behavior of Haynes 25 Co-base alloy was investigated in the temperature range of 950-1200 ˚C and 0.1 s-1. Thermodynamic calculations showed that M23C6 and M6C carbides were stable below 1000 ˚C and above 1050 ˚C, respectively. Stress-strain curves also indicated an unusual trend of strain fracture. It was observed that with increasing temperature from 950 to 105...

full text

Effects of Carbon on the Microstructure and Hot Deformation Behavior

The effects of carbon content on the dynamic and static softening mechanisms of Ti microalloy steels were investigated both in ferrite and austenite regions. &#10The results obtained showed that recrystallization rate decreased as the percentage of carbon content was increased from 0.0035 to 0.110. This is due to the Ti(CN) and TiC precipitates and also the free carbon content. In the ferrite r...

full text

Effects of Carbon on the Microstructure and Hot Deformation Behavior

The effects of carbon content on the dynamic and static softening mechanisms of Ti microalloy steels were investigated both in ferrite and austenite regions. The results obtained showed that recrystallization rate decreased as the percentage of carbon content was increased from 0.0035 to 0.110. This is due to the Ti(CN) and TiC precipitates and also the free carbon content. In the ferrite reg...

full text

Prediction of Temperature Distribution in the Hot Torsion Test Specimen

Hot torsion test (HTT) has extensively been used to analysis and physically model flow behavior and microstructure evolution of materials and alloys during hot deformation processes. In this test, the specimen geometry has a great influence in obtaining reliable test results. In this paper, the interaction of thermal-mechanical conditions and geometry of the HTT specimen was studied. The commer...

full text

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

full text

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 39  issue 3

pages  97- 113

publication date 2020-12

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

No Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023