Cyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy

Authors

  • Kourosh Shirvani Department of Advanced Materials and New Energies, Iranian Research Organization for Science and Technology (IROST), Tehran 15815-3538, Iran
  • Mohammad Farvizi Ceramic Division, Materials and Energy Research Center, Karaj, P.O. Box 31787-316, Iran
  • Mosleh Naderi Ceramic Division, Materials and Energy Research Center, Karaj, P.O. Box 31787-316, Iran
Abstract:

In this study, aluminide coating was employed to enhance the high-temperature cyclic oxidation of Rene-80 superalloy at 950ºC. The microstructural aspects and phase constituents of samples were  investigated with scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. The result of oxidation tests showed that the weight gain in the uncoated sample was considerably higher than the aluminide coated sample, which indicates the higher rate of oxide formation on the uncoated surface. With the aid of microstructural and XRD analysis, it was confirmed that with the increment of oxidation cycles, the thickness of aluminide coating reduced and the protective β-NiAl phase was converted to alumina scales. According to the EDS results taken from the top coat, it was found that with the increase of oxidation cycles, the content of aluminium in the top layer was drastically decreased and the weight percentage of oxygen was considerably enhanced. Also, in higher oxidation cycles, other protective elements such as Cr and Ti outwardly diffused from the inter-diffusion zone (IDZ) layer which led to reduction in the content of these elements in inner zones of the aluminide coating. 

Upgrade to premium to download articles

Sign up to access the full text

Already have an account?login

similar resources

Nickel Base Superalloy Rene®80 – The Effect of High Temperature Cyclic Oxidation on Platinum-Aluminide Coating Features

Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on beha...

full text

Cyclic oxidation-induced cracking of platinum-modified nickel-aluminide coatings

Short cracks, extending to the interdiffusion zone, have been observed in platinum-modified nickel-aluminide diffusion coatings on single-crystal CMSX-4 superalloys after these have been subject to short (10 min) rapid thermal cycles. The cracks were revealed after removing the thermally grown oxide formed during cycling on the coating surfaces. Cracking was observed for coatings subject to the...

full text

Formation and Evaluation of Oxidation Behavior of Zirconia- Aluminide Coating on Nickel- Based Alloy

Practical applications of thermal barrier coatings with aluminide bond-coats are limited due to oxide scale spallation of the aluminide coating under applied thermal stresses. Considering the positive effects of oxygen-active elements or their oxides on the high temperature oxidation behavior, in this research zirconia was introduced into an aluminide coating. For this purpose, a Watts type bat...

full text

Isothermal and cyclic oxidation behavior of AISI 430 ferritic stainless steel coated with titanium

In order to improve the oxidation resistance of ferritic stainless steel, it is possible to deposit a protective coating on steel substrate. In this research through the usage of pack cementation method a coating of titanium was applied on the surface of AISI 430 stainless steel. Scanning Electron-Microscopy (SEM), Energy- Dispersive X-ray spectrometry (EDAX) and X-ray diffraction (XRD) were us...

full text

On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings

The evolution of the surface roughness of an initially flat platinum-modified nickel aluminide (NiPtAl) coating on a single crystal superalloy with cyclic oxidation has been measured by optical profilometry and correlated with the aluminide microstructure. The roughness evolution is dominated by the relative motion of individual grains on thermal cycling, with the larger sized grains moving up ...

full text

The Effects of Beryllium Additions on the Oxidation of Nickel Aluminide and Titanium Aluminide Based Intermetallics

The effects of Be additions on the oxidation behavior of ~-NiAl in moist air at 1000°C and borderline alumina-forming y (TiAI) + Laves Ti-Al-Cr based alloys at 800°C and 1000°C in dry and moist air were investigated. The addition of Be to ~-NiAl suppressed the formation of transient alumina, and resulted in the formation of a protective BeAl20 4 spinel phase. In dry air, the addition of Be to t...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 4  issue Issue 3&4

pages  1- 7

publication date 2018-09-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023