preparation of nano gold powder from acid leaching tail solution

Authors

m. kargar razi

islamic azad university, north tehran branch, iran. m. khosravi

islamic azad university, north tehran branch, tehran,iran. r. sarraf mamoory

tarbiat modares university, tehran, iran. m. mohammadi

mouteh gold complex, iran.

abstract

according to the unique properties and many applications of nano gold powder, it was prepared from an acid leaching tail solution. the low value residual gold ions existed in acid leaching tail solution in mouteh gold mine in iran with fellow heavy metals as pollutants (fe2+, cu2+, and zn2+). preparation of nano gold particles is achieved by two steps: first, by addition of ammonia as separation step and second by using the suitable reagents for precipitation and extraction step. control conditions include ph, residence time, temperature, agitation, molar ratio of reducing agents to reagents. the optimum results show that nano gold powder was prepared by temperature of 250 °c, urea to gold molar ratio of 3:1, and reduction time of 20 min. also, heat treatment improves dispersion of nano sized gold particles. the properties of gold nano powders were evaluated by sem, a.a and uv-vis spectroscopy methods and the size of particles were about 80 to 90 nm.

Upgrade to premium to download articles

Sign up to access the full text

Already have an account?login

similar resources

Preparation of nano gold powder from acid leaching tail solution

According to the unique properties and many applications of nano gold powder, it was prepared from an acid leaching tail solution. The low value residual gold ions existed in acid leaching tail solution in Mouteh gold mine in Iran with fellow heavy metals as pollutants (Fe2+, Cu2+, and Zn2+). Preparation of nano gold particles is achieved by two steps: First, by addition of ammonia as separatio...

full text

Preparation of nano gold powder from acid leaching tail solution

According to the unique properties and many applications of nano gold powder, it was prepared from an acid leaching tail solution. The low value residual gold ions existed in acid leaching tail solution in Mouteh gold mine in Iran with fellow heavy metals as pollutants (Fe2+, Cu2+, and Zn2+). Preparation of nano gold particles is achieved by two steps: First, by addition of ammonia as separatio...

full text

Preparation of nano silver powder from acid leaching tail in gold room

According to the unique properties and many applications of nano silver powder, it was prepared from acid leaching tail solution. The low value residual gold and silver ions were occurred with fellow heavy metals as pollutants (Fe2+, Cu 2+ and Zn2+) in acid leaching tail solution in Mouteh gold mine in Iran. Preparation of nano silver particles was achieved in two steps: first, by addition of a...

full text

Preparation of nano silver powder from acid leaching tail in gold room

According to the unique properties and many applications of nano silver powder, it was prepared from acid leaching tail solution. The low value residual gold and silver ions were occurred with fellow heavy metals as pollutants (Fe2+, Cu 2+ and Zn2+) in acid leaching tail solution in Mouteh gold mine in Iran. Preparation of nano silver particles was achieved in two steps: first, by addition of a...

full text

preparation of nano silver powder from acid leaching tail in gold room

according to the unique properties and many applications of nano silver powder, it was prepared from acid leaching tail solution. the low value residual gold and silver ions were occurred with fellow heavy metals as pollutants (fe2+, cu 2+ and zn2+) in acid leaching tail solution in mouteh gold mine in iran. preparation of nano silver particles was achieved in two steps: first, by addition of a...

full text

Preparation of Fe3Si/Ferrite Micro- and Nano-Powder Composite

Composite material based on Fe3Si micro-particles and Mn-Zn nano-ferrite was prepared using powder metallurgy technology. The sol-gel followed by autocombustion process was used for synthesis of Mn0.8Zn0.2Fe2O4 ferrite. 3 wt.% of mechanically milled ferrite was mixed with Fe3Si powder alloy. Mixed micro-nano powder system was homogenized by the Resonant Acoustic Mixing using ResodynLabRAM Mixer...

full text

My Resources

Save resource for easier access later


Journal title:
international journal of nano dimension

جلد ۱، شماره ۱، صفحات ۴۷-۵۵

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023