Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods
نویسندگان
چکیده
1Universidade Tiradentes – UNIT, School of Dentistry, Department of Oral Rehabilitation, Aracaju, SE, Brazil 2Universidade Estadual Paulista – UNESP, School of Dentistry, Department of Dental Materials and Prosthodontics, Araraquara, SP, Brazil 3Universidade Potiguar UnP, School of Dentistry, Department of Oral Rehabilitation, Natal, RN, Brazil 4Universidade do Estado do Rio de Janeiro – UERJ, Resende School of Technology, Department of Engineering Materials, Resende, RJ, Brazil
منابع مشابه
Effect of resin cement selection on the microtensile bond strength of adhesively veneered 3Y-TZP.
OBJECTIVE The aim of this study was to investigate the effect of resin cement selection on the microtensile bond strength (μTBS) of adhesively veneered 3Y-TZP. MATERIALS AND METHODS 3Y-TZP discs were fabricated from commercial powders and treated by sandblasting and zirconia primer. Porcelain discs were sectioned from a feldspathic block and conditioned with 5% HF and silane agent. Pre-treate...
متن کاملLow-Fusing Porcelain Glaze Application on 3Y-TZP Surfaces can Enhance Zirconia-Porcelain Adhesion.
The aim of this study was to assess whether surface treatment improves zirconia-porcelain adhesion. The 3Y-TZP blocks were cut into squares, then polished and sintered. The zirconia surface treatments were performed as follows: no treatment (C); tribochemical silica coating (TBS); glaze application + hydrofluoric acid etching (GA); glaze application + hydrofluoric acid etching + silanization (G...
متن کاملEffects of extreme cooling methods on mechanical properties and shear bond strength of bilayered porcelain/3Y-TZP specimens.
OBJECTIVES This study investigated the effect of extreme cooling methods on the flexural strength, reliability and shear bond strength of veneer porcelain for zirconia. METHODS Vita VM9 porcelain was sintered on zirconia bar specimens and cooled by one of the following methods: inside a switched-off furnace (slow), at room temperature (normal) or immediately by compressed air (fast). Three-po...
متن کاملHighly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation.
Latest trends in dental restorative ceramics involve the development of full-contour 3Y-TZP ceramics which can avoid chipping of veneering porcelains. Among the challenges are the low translucency and the hydrothermal stability of 3Y-TZP ceramics. In this work, different trivalent oxides (Al2O3, Sc2O3, Nd2O3 and La2O3) were selected to dope 3Y-TZP ceramics. Results show that dopant segregation ...
متن کاملEffect of bracket base design on shear bond strength to feldspathic porcelain
OBJECTIVES This study sought to assess the effect of bracket base design on the shear bond strength (SBS) of the bracket to feldspathic porcelain. MATERIALS AND METHODS This in vitro, experimental study was conducted on 40 porcelain-fused-to-metal restorations and four different bracket base designs were bonded to these specimens. The porcelain surfaces were etched, silanized, and bonded to b...