Dopant depth profiling and dose determination are essential for ultrashallow junction technology development. However they pose a challenge to the widely used dynamic secondary ion mass spectroscopy SIMS technique that suffers uncertainties due to an initial transient width comparable to the dopant depth distribution. In this work the authors report on the application of grazing incidence x-ray fluorescence GIXRF for arsenic in silicon dose and profile determination and its combination with SIMS in order to try to overcome the limitations of the latter in the topmost few nanometers. A polynomial variation of the sputtering rate is supposed in the first sputtering stage of the SIMS analysis and the parameters that regulate the magnitude of such correction are determined by a least square fitting of the angle dependent fluorescence signal. The total retained fluence was also measured by instrumental neutron activation analysis and synchrotron radiation soft x-ray GIXRF. The comparison among the total retained fluence determinations shows a good agreement among the techniques. Furthermore, from this first set of measurements it was clearly shown that the GIXRF profile correction is very sensitive to the SIMS profile in the very first nanometers. Therefore if matrix effects are present in the SIMS analysis beside the sputtering rate change, the tested sputtering rate correction can produce nonreliable profiles. © 2010 American Vacuum Society. DOI: 10.1116/1.3292647

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Deactivation of submelt laser annealed arsenic ultrashallow junctions in silicon during subsequent thermal treatment

The use of nonequilibrium annealing approaches can produce very high levels of arsenic electrical activation in Si. However, subsequent thermal treatments between 500 and 800 °C easily deactivate the dopant to a level one order of magnitude below the solid solubility. In this work, the authors study the deactivation of laser annealed LA ultrashallow arsenic distributions in silicon using Hall e...

متن کامل

Depth profiling of low energy ion implantations in Si and Ge by means of micro-focused grazing emission X-ray fluorescence and grazing incidence X-ray fluorescence

Depth-profiling measurements by means of synchrotron radiation based grazing XRF techniques, i.e., grazing emission X-ray fluorescence (GEXRF) and grazing incidence X-ray fluorescence (GIXRF), present a promising approach for the non-destructive, sub-nanometer scale precision characterization of ultra shallow ion-implantations. The nanometer resolution is of importance with respect to actual se...

متن کامل

Determining the Content of Silicon Dioxide in Bauxites Using X-Ray Fluorescence Spectrometry

The X-ray fluorescence spectrometry and the MA.BM.006 reference spectrophotometric methods were used to determine the content of SiO2 (%) in bauxites from different deposits. The treatment of samples prior to the analysis involved the following steps: annealing, melting using the borax method,  and the formation of beads. Certified reference bauxite samples were used for the cali...

متن کامل

Nanoscale Junction Formation by Gas-Phase Monolayer Doping.

A major challenge in transistor technology scaling is the formation of controlled ultrashallow junctions with nanometer-scale thickness and high spatial uniformity. Monolayer doping (MLD) is an efficient method to form such nanoscale junctions, where the self-limiting nature of semiconductor surfaces is utilized to form adsorbed monolayers of dopant-containing molecules followed by rapid therma...

متن کامل

Differential Hall effect profiling of ultrashallow junctions in Sb implanted silicon

A differential Hall effect technique has been developed to obtain doping profiles at a depth resolution down to 2 nm with junction depths of about 20 nm. We have determined the electrical characteristics of 531014 Sb+ cm−2 implanted in (100) silicon at an energy of 5 keV. A comparison was made between carrier concentration profiles and secondary ion mass spectroscopy measurements of the atomic ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2010