Objectives. This study evaluated the influence of cavity surface finishing with diamond burs of different grit mounted on high-speed turbine and ultrasound on the roughness and microshear bond strength (MBS) of a lithium silicate glass-ceramic to enamel and dentin. Methods. Enamel and dentin specimens were divided into seven groups, according to the type of surface finishing: 1200-grit sandpaper (control), two different brands of medium-grit and fine-grit diamond burs in a high-speed turbine; medium-grit and fine-grit CVD (chemical vapor deposition) tips in an ultrasonic device. Roughness parameters (n = 5) and MSBS to a glass-ceramic (n = 10) were determined. Data were analyzed using ANOVA and Tukey's test (α = 5%). Results. Control group showed lower mean roughness readings and groups that used medium-grit diamond burs showed the highest mean roughness values. Regarding MSBS, there was no statistical difference when comparing the groups gritted with the same brand of medium- and fine-grit burs and tips. Conclusions. Cavity surface finishing influenced the roughness parameters and MSBS of a glass-ceramic to enamel and dentin. Medium-grit diamond burs in high-speed turbine showed the highest mean roughness values. Fine-grit CVD tips in ultrasound presented the highest MSBS values for both enamel and dentin.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microshear Bond Strength of Glass Ionomer to Primary Dentin following Surface Treatment by Bur and Er,Cr:YSGG Laser

Background and Aim: Er,Cr:YSGG laser irradiation has been suggested as an effective method of cavity preparation and surface treatment to enhance the bond strength. The aim of this study was to assess the microshear bond strength of Fuji II LC glass ionomer (GI) cement to primary dentin following bur preparation and Er,Cr:YSGG irradiation. Materials and Methods: This in vitro, experimental stu...

متن کامل

Effect of Er:YAG Laser Irradiation on Shear Bond Strength of Two Porcelain Laminate Veneers Bonded to Tooth Surface

Background and Aim: The conventional procedure for removal of porcelain laminate veneers (PLVs) is time-consuming and inconvenient. The purpose of this study was to evaluate the efficacy of Er:YAG laser for debonding of PLVs. Materials and Methods: Forty-eight intact extracted human maxillary anterior teeth received discoid PLVs (24 feldspathic and 24 e-max ceramic). The PLVs had 0.7 mm thickn...

متن کامل

The Effect of Lithium Disilicate Ceramic Thickness and Translucency on Shear Bond Strength of Light-cured Resin Cement

Introduction: To achieve acceptable clinical performance, a ceramic veneer must be bonded to enamel by well-polymerized resin cement. Among different factors, thickness and translucency of the ceramic may affect the resin cement polymerization. Thus, the current study evaluated the effect of the thickness and translucency of lithium disilicate ceramic on light-cured resin cement bond strength t...

متن کامل

بررسی اثر تعداد لایه‌های ادهزیو بر استحکام باند ریز برشی و ریز سختی سطح باند شده عاج پس از کاربرد چهار نوع ادهزیو

Background and Aims: In this in-vitro study, the effect of multiple adhesive coating on the microshear bond strength of composite to dentin and surface microhardness of dentin after treatment with four adhesives (One Step Plus, One Step, Single Bond, Single Bond 2) were evaluated. Materials and Methods: One hundred intact human molars were cut to obtain disks of dentin having 2 mm thickness. F...

متن کامل

Effect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown

This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 2015  شماره 

صفحات  -

تاریخ انتشار 2015