BACKGROUND Most contemporary total disc replacements (TDRs) use conventional orthopaedic bearing couples such as ultrahigh-molecular-weight polyethylene (polyethylene) and cobalt-chromium (CoCr). Cervical total disc replacements incorporating polyetheretherketone (PEEK) bearings (specifically PEEK-on-PEEK bearings) have been previously investigated, but little is known about PEEK-on-ceramic bearings for TDR. QUESTIONS/PURPOSES (1) What is the tribologic behavior of a PEEK-on-ceramic bearing for cervical TDR under idealized, clean wear test conditions? (2) How does the PEEK-on-ceramic design perform under impingement conditions? (3) How is the PEEK-on-ceramic bearing affected by abrasive wear? (4) Is the particle morphology from PEEK-on-ceramic bearings for TDRs affected by adverse wear scenarios? METHODS PEEK-on-ceramic cervical TDR bearings were subjected to a 10 million cycle ideal wear test based on ASTM F2423 and ISO 181912-1 using a six-station spine wear simulator (MTS, Eden Prairie, MN, USA) with 5 g/L bovine serum concentration at 23° ± 2° C (ambient temperature). Validated 1 million cycle impingement and 5 million cycle abrasive tests were conducted on the PEEK-on-ceramic bearings based, in part, on retrieval analysis of a comparable bearing design as well as finite element analyses. The ceramic-on-PEEK couple was characterized for damage modes, mass and volume loss, and penetration and the lubricant was subjected to particle analysis. The resulting mass wear rate, volumetric wear rate, based on material density, and particle analysis were compared with clinically available cervical disc bearing couples. RESULTS The three modes of wear (idealized, impingement, and abrasive) resulted in mean mass wear rates of 0.9 ± 0.2 mg/MC, 1.9 ± 0.5 mg/MC, and 2.8 ± 0.6 mg/MC, respectively. The mass wear rates were converted to volumetric wear rates using density and found to be 0.7 ± 0.1 mm3/MC, 1.5 ± 0.4 mm3/MC, and 2.1 ± 0.5 mm3/MC, respectively. During each test, the PEEK endplates were the primary sources of wear and demonstrated an abrasive wear mechanism. Under idealized and impingement conditions, the ceramic core also demonstrated slight polishing of the articulating surface but the change in mass was unmeasurable. During abrasive testing, the titanium transfer on the core was shown to polish over 5 MC of testing. In all cases and consistent with previous studies of other PEEK bearing couples, the particle size was primarily < 2 µm and morphology was smooth and spheroidal. CONCLUSIONS Overall, the idealized PEEK-on-ceramic wear rate (0.7 ± 0.1 mm3/MC) appears comparable to the published wear rates for other polymer-on-hard bearing couples (0.3-6.7 mm3/MC) and within the range of 0.2 to 1.9 mm3/MC reported for PEEK-on-PEEK cervical disc designs. The particles, based on size and morphology, also suggest the wear mechanism is comparable between the PEEK-on-ceramic couple and other polymer-on-ceramic orthopaedic couples. CLINICAL RELEVANCE The PEEK-on-ceramic bearing considered in this study is a novel bearing couple for use in total disc arthroplasty devices and will require clinical evaluation to fully assess the bearing couple and total disc design. However, the wear rates under idealized and adverse conditions, and particle size and morphology, suggest that PEEK-on-ceramic bearings may be a reasonable alternative to polyethylene-on-CoCr and metal-on-metal bearings currently used in cervical TDRs.
منابع مشابه
Contemporary Ceramic Total Hip Arthroplasty in Patients with Cerebral Palsy: Does It Work?
BACKGROUND Adult patients with cerebral palsy (CP), who have advanced degenerative arthritis of the hip, have been treated with resection arthroplasty and arthrodesis. Although total hip arthroplasty (THA) has also been used as one of the alternative options, there are few studies on contemporary bearings used in THA. Therefore, we evaluated the results of the contemporary ceramic-on-ceramic TH...
متن کاملWear of ceramic-on-carbon fibre reinforced PEEK hip replacements
Total hip replacement has been a successful surgical intervention for many years. However, concerns regarding UHMWPE wear particle induced osteolysis [1], have led to alternative bearing materials to be sought. Carbon-fibre reinforced poly-ether-ether-ketone (CFR-PEEK) is a fibre-reinforced polymer which has shown reduced wear in hip and knee configurations compared with conventional polyethyle...
متن کاملFracture of ceramic components as a serious failure after total hip replacement with ceramic-on-ceramic bearings
Introduction Ceramics have been introduced in total hip arthroplasty for several advantages including minimal friction, low wear, biocompatibility, no ageing problems and no problems related to the systemic increases in serum metal concentrations. In the first generation of ceramic components introduced in the 1970’s the risk of fracture was substantial, reaching up to 13.4 %. After introducing...
متن کاملComparison of the risk of revision in cementless total hip arthroplasty with ceramic-on-ceramic and metal-on-polyethylene bearings
BACKGROUND AND PURPOSE Ceramic-on-ceramic (CoC) bearings were introduced in total hip arthroplasty (THA) to reduce problems related to polyethylene wear. We compared the 9-year revision risk for cementless CoC THA and for cementless metal-on-polyethylene (MoP) THA. PATIENTS AND METHODS In this prospective, population-based study from the Danish Hip Arthroplasty Registry, we identified all the...
متن کاملThe Use of Ceramics in Total Hip Arthroplasty
Ceramics have excellent mechanical properties and very stable wear characteristics and therefore have been used in many industries including automotives, aeronautics and healthcare. The use of ceramics in total hip arthroplasty has been increasing. This review article we will provide an overview of where we started and how far we have come. We will review the mechanical properties of ceramics, ...