Laser Engineered Net Shaping of Nickel-Based Superalloy Inconel 718 Powders onto AISI 4140 Alloy Steel Substrates: Interface Bond and Fracture Failure Mechanism

نویسندگان

  • Hoyeol Kim
  • Weilong Cong
  • Hong-Chao Zhang
  • Zhichao Liu
چکیده

As a prospective candidate material for surface coating and repair applications, nickel-based superalloy Inconel 718 (IN718) was deposited on American Iron and Steel Institute (AISI) 4140 alloy steel substrate by laser engineered net shaping (LENS) to investigate the compatibility between two dissimilar materials with a focus on interface bonding and fracture behavior of the hybrid specimens. The results show that the interface between the two dissimilar materials exhibits good metallurgical bonding. Through the tensile test, all the fractures occurred in the as-deposited IN718 section rather than the interface or the substrate, implying that the as-deposited interlayer bond strength is weaker than the interfacial bond strength. From the fractography using scanning electron microscopy (SEM) and energy disperse X-ray spectrometry (EDS), three major factors affecting the tensile fracture failure of the as-deposited part are (i) metallurgical defects such as incompletely melted powder particles, lack-of-fusion porosity, and micropores; (ii) elemental segregation and Laves phase, and (iii) oxide formation. The fracture failure mechanism is a combination of all these factors which are detrimental to the mechanical properties and structural integrity by causing premature fracture failure of the as-deposited IN718.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Tensile Fracture Behavior and Failure Mechanism of Additively-Manufactured AISI 4140 Low Alloy Steel by Laser Engineered Net Shaping

AISI 4140 powder was directly deposited on AISI 4140 wrought substrate using laser engineered net shaping (LENS) to investigate the compatibility of a LENS-deposited part with the substrate. Tensile testing at room temperature was performed to evaluate the interface bond performance and fracture behavior of the test specimens. All the samples failed within the as-deposited zone, indicating that...

متن کامل

Nickel-based Superalloy Layer Deposited on AISI H13 Hot Tool Steel Base Metal Using Explosion Cladding process

An experimental test was carried out to explosively clad solution annealed Inconel 718 superalloy on quench-tempered AISI H13 hot tool steel. A wavy with vortices interface geometry was obtained from this experiment. A gradual change in the wavelength along the direction of welding was observed which was due to a change in the impact angle, following the plate contacts. In this paper, the exper...

متن کامل

MICROSTRUCTURAL STUDIES ON LASER WELDING OF INCONEL 718 TO 2304 DUPLEX STAINLESS STEEL WITH A FOCUS ON OPTIMAZING PROCESS PARAMETERS AND ACHIEVING THE MAXIMUM FRACTURE STRENGTH

In this research, microstructure and mechanical properties of laser welded joints between 2304 duplex stainless steel and Inconel 718 nickel-based super alloy were investigated. Microstructural evolution in the various areas of welded joints and also the effect of welding parameters on the mechanical properties of dissimilar joints were studied. Response surface methodology based on the central...

متن کامل

AN EVALUATION OF THERMAL STABILITY IN DISSIMILAR WELDS BETWEEN 310 STAINLESS STEEL AND ALLOY 657

Abstract: The investigation is carried out to characterize welding of AISI 310 austenitic stainless steel to Inconel 657 nickel-chromium superalloy. The welds were produced using four types of filler materials: the nickel-based corresponding to Inconel 82, Inconel A, Inconel 617 and austenitic stainless steel 310. This paper describes the effects of aging treatment on the joint. The compara...

متن کامل

Evaluation of microstructure and corrosion behavior of dissimilar laser joint between Inconel 625 and AISI 430 ferritic stainless steel

Dissimilar weld joints between stainless steels and nickel based super alloys are extensively used in petrochemical, gas and oil applications. These joints jave great challenges from metallurgical transformations point of view. In this research, microstructural evolutions and corrosion behavior of laser weld joint between Inconel 625 and AISI 430 ferritic stainless steel were investigated. Ferr...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 10  شماره 

صفحات  -

تاریخ انتشار 2017