Study on Corrosion Behavior of Pearlitic Rail Steel
نویسنده
چکیده
The present study is an attempt to find out the effect of environmental corrosion on the commonly used pearlitic rail steel. The cases of corrosion of rail under Indian environment have been studied. It has been found that in marine environment both the yield strength and tensile strength decreases with increasing corrosion rate. In acidic environment yield strength increased with increasing corrosion rate, although the tensile strength decreases with increasing corrosion rate.
منابع مشابه
Corrosion of Different Materials in Combustion Chamber of Yellow Phosphorus Tail Gas in Industrial Boiler
About 75% of yellow phosphorus produced in the world is from China, and Yunnan province produces 60% of that in China. Yellow phosphorus is mostly produced by electric furnace from phosphate minerals. Through this method, 2500-3000 Nm/t tail gas is emitted, which causes pollution of the atmosphere. The key composition of the tail gas contains 80%~95%CO. Due to the “3R” principle (reducing, reus...
متن کاملAn Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution
The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...
متن کاملInvestigating the Effect of the Deep Cryogenic Heat Treatment on the Mechanical Properties and Corrosion Behavior of 1.2080 Tool Steel
Deep cryogenic heat treatment is assumed as a supplementary heat treatment performed on steels before the final tempering treatment to enhance the wear resistance and hardness of the steels. In this study, the effects of the deep cryogenic heat treatment on the wear behavior and corrosion resistance of the 1.2080 tool steel were studied using the wear testing machine and polarization and impeda...
متن کاملSynthesis of syntactic steel foam using gravity-fed infiltration
In this study, we report a procedure for producing syntactic steel foams by melt infiltration of millimeter-sized ceramic microspheres. The gravity-fed infiltration method yields steel foam with uniform distributions of microspheres and negligible unintended porosity. The critical parameters in the manufacturing process are the melt temperature and the preheat temperature of the microspheres pr...
متن کاملInvestigation on Effect of Heat Input on the Corrosion Behavior of Hadfield Steel Weld Joints in SMAW Process
In this investigation, the effect of heat input of SMAW process on the corrosion behavior of Hadfield steel weld joints was investigated. For this purpose, 4 annealed sheets with thickness 25 mm prepared from Hadfield steel and then welding applied by SMAW process with 6.75 and 11.25 kJ/mm heat input values. For corrosion behavior evaluation of base metal and weld metal areas, potentiodynamic p...
متن کامل