Fatigue Behaviour of Al 6082-T6 Friction Stir Welded Tubular Joints under Torsional Loading
نویسندگان
چکیده
The aim of the present research is to investigate the fatigue behaviour of friction stir (FS) welded tubular joints in aluminium alloy subjected to torsional fatigue loading. To manufacture the samples which were tested, an MTS I-STIR process development system was equipped with a retracting tool specifically designed for these tubular welds. Al 6082-T6 FS welded samples were tested under cyclic torsion with a nominal shear stress ratio equal to -1 and 0. The test data show that, strictly speaking, the presence of non-zero mean shear stresses has a detrimental effect on the overall torsional fatigue strength of the FS welded joints. However, the reanalysis discussed in the present paper suggests that, from a statistical point of view, any detrimental effect is small. This means that fatigue assessment under torsional fatigue loading of these FS welded tubular connections can be performed with little loss of accuracy by neglecting the presence of non-zero mean shear stresses.
منابع مشابه
Fatigue Life of Repaired Welded Tubular Joints
In this study, the effect of repair on fatigue life of tubular joints is investigated. Six cracked specimens precedently subjected to fatigue loading undergone to weld repair. Two of those specimens were shot peened before primary fatigue loading. It is shown that repair gives rise to about 150% increase in fatigue life for original specimens while the increase of fatigue life for shot-peened ...
متن کاملEffect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys
In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observati...
متن کاملEffect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys
In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observati...
متن کاملEffect of heat treatment on the grain structure and mechanical properties of Al-7075 friction stir weld
The fine grain structure of friction-stir welded aluminum alloys is unstable during post weld heat treatment and some grains abnormally grown. In this study, the sequence of abnormal grain growth during T6 heat treatment of Al-7075 friction-stir weld and its effect on mechanical properties of the weld was studied. The results showed that heat treatment in 510 ˚C resulted in drastic grain growth...
متن کاملInvestigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method
In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...