Dielectric relaxation and pinning phenomenon of (Sr,Pb)TiO3 ceramics for dielectric tunable device application

نویسندگان

  • Xian-Xiong Huang
  • Tian-Fu Zhang
  • Xin-Gui Tang
  • Yan-Ping Jiang
  • Qiu-Xiang Liu
  • Zu-Yong Feng
  • Qi-Fa Zhou
چکیده

The behavior of ferroelectric domain under applied electric field is very sensitive to point defects, which can lead to high temperature dielectric relaxation behaviors. In this work, the phases, dielectric properties and ferroelectric switching behavior of strontium lead titanate ceramics were investigated. The structural characterization is confirmed by X-ray diffraction. The high dielectric tunability and high figure of merit of ceramics, especially Sr0.7Pb0.3TiO3 (SPT), imply that SPT ceramics are promising materials for tunable capacitor applications. Oxygen vacancies induced dielectric relaxation phenomenon is observed. Pinched shape hysteresis loops appeared in low temperature, low electric field or high frequency, whereas these pinched hysteresis loops also can become normal by rising temperature, enhancing electric field or lowering frequency. The pinning and depinning effect can be ascribed to the interaction between oxygen vacancies and domain switching. A qualitative model and a quantitative model are used to explain this phenomenon. Besides, polarization and oxygen treated experiment can exert an enormous influence on pinning effect and the machanisms are also discussed in this work.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Diffuse dielectric anomaly in perovskite-type ferroelectric oxides in the temperature range of 400–700°C

The diffuse dielectric anomaly by the dielectric relaxation found at the high-temperature region of 400–700 °C was investigated in perovskite-type ferroelectric oxides such as BaTiO3 , (Pb,La!TiO3 , and (Pb,La!~Zr,Ti!O3 ceramics. We observed that the diffuse dielectric anomaly in perovskite oxides was strongly affected by oxygen-related processing parameters. We have modified the Debye relaxati...

متن کامل

Improved Figure of Merit of (Ba,Sr)TiO3-Based Ceramics by Sn Substitution

The dielectric properties of (Ba0:6Sr0:4)(Ti1 xSnx )O3 (0 x 0:3) ceramics were investigated. Single-phase specimens having a cubic perovskite structure could be obtained. As Sn concentration increased, dielectric loss decreased untill a composition of x 1⁄4 0:15 and slightly increased as Sn concentration increased further. The diffused phase transition appeared owing to substitution of Sn ions....

متن کامل

Dielectric Relaxation in Ceramics with Intragrain Concentration Gradient

We created a material with a composition gradient within each grain. Due to the graded composition the ceramic does not show a sharp change in dielectric constant near the relaxation frequency. Instead, we observe gradual decrease in dielectric constant with frequency, with the loss tangent remaining practically unchanged (below 0.02 everywhere within the frequency range 0.0003-3 GHz). The tuna...

متن کامل

Dielectric behavior of paraelectric KTaO3 , CaTiO3, and „Ln1Õ2Na1Õ2...TiO3 under a dc electric field

The dc electric-field dependence of dielectric constant in the paraelectrics, KTaO3 single crystals, CaTiO3 and (Ln1/2Na1/2)TiO3 (Ln5La and Nd! ceramics is studied at cryogenic temperatures in the dc electric-field range 0–60 kV/cm. The results indicate that KTaO3 possesses a high tunability K$5@e(E0)2e(E)#/e(E0) 5;50%% at 20 kV/cm, and low dielectric loss tan d (;0.003); while CaTiO3 and (Ln1/...

متن کامل

Processing and Characterization of Microwave Dielectric Ceramics and Thin Films-Nd2(Ti2/3Al1/3)3O9-δ and (Ba0.7Sr0.3)TiO3

Reactive powders of stoichiometry Nd2(Ti2/3Al1/3)3O9-δ and thin films of (Ba0.7Sr0.3)TiO3 have been prepared by the conventional mixed-oxide method and the metal-organic deposition method, respectively. The corresponded phases after calcination and sintering are investigated by XRD diffraction. Single phase of Nd2(Ti2/3Al1/3)3O9-δ could be only obtained by sintering over 1400C for 4 h. (Ba0.7Sr...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 6  شماره 

صفحات  -