Differences in the force system delivered by different beta-titanium wires in elaborate designs

نویسندگان

  • Renato Parsekian Martins
  • Sergei Godeiro Fernandes Rabelo Caldas
  • Alexandre Antonio Ribeiro
  • Luís Geraldo Vaz
  • Roberto Hideo Shimizu
  • Lídia Parsekian Martins
چکیده

OBJECTIVE Evaluation of the force system produced by four brands of b-Ti wires bent into an elaborate design. METHODS A total of 40 T-loop springs (TLS) hand-bent from 0.017 x 0.025-in b-Ti were randomly divided into four groups according to wire brand: TMATM(G1), BETA FLEXYTM (G2), BETA III WIRETM (G3) and BETA CNATM (G4). Forces and moments were recorded by a moment transducer, coupled to a digital extensometer indicator adapted to a testing machine, every 0.5 mm of deactivation from 5 mm of the initial activation. The moment-to-force (MF) ratio, the overlapping of the vertical extensions of the TLSs and the load-deflection (LD) ratio were also calculated. To complement the results, the Young's module (YM) of each wire was determined by the slope of the load-deflection graph of a tensile test. The surface chemical composition was also evaluated by an energy dispersive X-ray fluorescence spectrometer. RESULTS All groups, except for G2, produced similar force levels initially. G3 produced the highest LD rates and G1 and G4 had similar amounts of overlap of the vertical extensions of the TLSs in "neutral position". G1 and G3 delivered the highest levels of moments, and G2 and G3 produced the highest MF ratios. b-Ti wires from G3 produced the highest YM and all groups showed similar composition, except for G2. CONCLUSION The four beta-titanium wires analyzed produced different force systems when used in a more elaborate design due to the fact that each wire responds differently to bends.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of mechanical properties of beta-titanium wires between leveled and unleveled brackets: an in vitro study

BACKGROUND The objective of this study is to evaluate the force-deflection behavior of beta-titanium alloy wires between two leveled and unleveled bracket alignment scenarios using a three-point bending test. METHODS Six groups of ten beta-titanium alloy wire segments (0.017 × 0.025-in. diameter) of different manufacturers (Orthometric, Ortho Organizers, GAC, Morelli, and Ormco) were used. Bo...

متن کامل

Comparison of the superelasticity of different nickel–titanium orthodontic archwires and the loss of their properties by heat treatment

The aim of this work is to describe and compare mechanical properties of eight widely used nickel-titanium orthodontic wires under uniform testing conditions and to determine the influence of the heat treatments on the loss of the superelasticity. Ten archwires from two batches from eight different manufacturers were evaluated. A three-point bending test was performed, in accordance with ISO 15...

متن کامل

Frictional resistance of self-ligating versus conventional brackets in different bracket-archwire-angle combinations

OBJECTIVE To compare the influence of archwire material (NiTi, beta-Ti and stainless steel) and brackets design (self-ligating and conventional) on the frictional force resistance. MATERIAL AND METHODS Two types of brackets (self-ligating brackets - Smartclip, 3M/Unitek - and conventional brackets - Gemini, 3M/Unitek) with three (0, 5, and 10 degrees) slot angulation attached with elastomeric...

متن کامل

Frictional forces related to self-ligating brackets.

Orthodontic tooth movement can be regarded as teeth sliding on a wire like pearls on a string, the force being supplied by springs or elastics. The movement implies friction between wire and bracket, taking up part of the force and leaving an uncontrolled amount to act on the teeth. The friction is likely to depend on bracket construction and wire material. Therefore, in this investigation the ...

متن کامل

Surface roughness of orthodontic wires via atomic force microscopy, laser specular reflectance, and profilometry.

The surface roughness of orthodontic archwires is an essential factor that determines the effectiveness of arch-guided tooth movement. Using the non-destructive techniques of atomic force microscopy (AFM) and of laser specular reflectance, the surface roughness of 11 nickel-titanium orthodontic wires, a stainless steel and a beta-titanium wire was measured. The results were compared with those ...