Bonding to Different PEEK Compositions: The Impact of Dental Light Curing Units
نویسندگان
چکیده
This study investigated the impact of different light curing units (LCUs) for the polymerization of adhesive system visio.link (VL) on the tensile bond strength (TBS) of different PEEK compositions. For TBS measurements, 216 PEEK specimens with varying amounts of TiO₂ (PEEK/0%, PEEK/20%, PEEK/>30%) were embedded, polished, air abraded (Al₂O₃, 50 µm, 0.4 MPa), conditioned using VL, and polymerized using either a halogen LCU (HAL-LCU) or a LED LCU (LED-LCU) for chairside or labside application, respectively. After thermocycling (5000×, 5/55 °C), TBS was measured, and fracture types were determined. Data was analyzed using a 2-way ANOVA followed by Tukey-HSD, Kruskal-Wallis H and Mann-Whitney U tests as well as a Chi²-test and a Ciba-Geigy table (p < 0.05). Globally, the light curing units, followed by PEEK composition, was shown to have the highest impact on TBS. The HAL-LCUs, compared to the LED-LCUs, resulted in a higher TBS for all PEEK compositions-without significant differences between chairside and labside units. Regarding the different PEEK compositions, PEEK/20%, compared to PEEK/0%, resulted in a higher TBS when both, HAL-LCUs or LED-LCUs were used for labside application. In comparison with PEEK/>30%, PEEK/20% resulted in a higher TBS after using HAL-LCU for labside application. No significant differences were found between PEEK/0% and PEEK/>30%. HAL-LCU with PEEK/20% for labside application showed a higher TBS than HAL-LCU with PEEK/20% for chairside application, whereas LED-LCU with PEEK/>30% for chairside application showed a higher TBS than LED-LCU with PEEK/>30% for labside application.
منابع مشابه
Evaluation of Microleakage in Fissure Sealants following Contamination with Artificial Saliva at Different Curing Times with or without using bonding agent
Background and Aim: One of the important factors in microleakage of fissure sealants is saliva contamination. Researchers believe that applying bonding agents can reduce the microleakage. The present study compared the microleakage of a fissure sealant contaminated with artificial saliva at different curing times with or without using a bonding agent. Materials and Methods: In this in-vitro ...
متن کاملEffect of thermal cycling on microleakage of a fissure sealant polymerized with different light sources.
The purpose of this study was to examine the effect of thermal cycling on microleakage of a fissure sealant after it was bonded with different bonding agents and polymerized with different light curing units. To this end, two bonding agents (Xeno III, iBond), three light curing units (Astralis 3, Elipar free-light, Elipar free-light 2), and a fissure sealant (Fissurit FX) were used. Microleakag...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light ...
متن کاملبررسی کارائی دستگاههای لایتکیور در مطبهای دندانپزشکی خصوصی شهر تهران در سال 1384
Background and Aim: Light cured composites and other restorative materials are quite common in dentistry today. Successful restorations are dependent on efficiency of curing light unit, eg. the intensity of emitted light and its wave length. The aim of this study was to evaluate the efficiency units of curing, in private dental offices in Tehran. Materials and Methods: In this descriptive cross...
متن کاملThe Effect of Standard and Extended Curing Time in Different Distances on Composite’s Degree of Conversion
Introduction: The aim of this study was to in-vestigate the effect of irradiation duration and distance of light tip to prepared samples in two different light curing unites on the degree of conversion of resin composite. Materials and Methods: Conventional halogen and blue Light emitting diode (LED) units were used for polymerization of an Opalis resin com-posite. The conversion measurements w...
متن کامل