Impact Behavior of Three Notched All-Ceramic Restorations after Soaking in Artificial Saliva

نویسندگان

  • Min Yan
  • Chung-Kai Wei
  • Yuh-Yih Lin
  • Suh-Woan Hu
  • Shinn-Jyh Ding
چکیده

Biomechanics play a critical role in influencing the clinical applications of all-ceramic dental restorations. The restorative biomaterials have to demonstrate mechanical durability in the oral environment because they are always exposed to a variety of oral environments. This study was designed to evaluate the effect of soaking time, notch and saliva pH values on the impact energy of three commonly used all-ceramic materials for CAD/CAM. The leucite-reinforced glass ceramic (ProCAD), lithium disilicate glass ceramic (IPS e.max CAD) and zirconia-based ceramic materials (IPS e.max ZirCAD) were used. The experimental results indicated that the impact energy of ProCAD decreased with an increase in soaking time, but not for IPS e.max CAD and IPS e.max ZirCAD. The impact energy of the zirconia system was higher than leucite-reinforced and lithium disilicate-based ceramic systems. When subjected to preformed 0.5 mm U-shape notch on the bar specimen of 3 mm thick, the impact energy of the all-ceramic restorations revealed a markedly reduction of about 80%-90%, almost irrespective of dental compositions, which indicated the effect of flaw to a great degree. No statistically significant influence (p > 0.05) of pH values (4, 7 and 9) on impact energy was found for each group. It is concluded that the no matter which all-ceramic materials were used, it was appreciably sensitive to the presence of notches. The ceramic composition and microstructure have been shown to affect mechanical durability.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Influence of Various Mucoadhesive Polymers on In Vitro Performance of the Resulting Artificial Saliva Pump Spray Formulations

The aim of this study was to investigate the rheological behavior and mucoadhesive nature of saliva substitutes, by incorporating various mucoadhesive polymers into an artificial saliva pump spray formulation. For this purpose various mucoadhesive polymers including cellulosic polymers in the range of 0.1-1.0% and Carbomers such as C974p, C971, C934p and C971 in the range of 0.01-0.1% were adde...

متن کامل

The Influence of Various Mucoadhesive Polymers on In Vitro Performance of the Resulting Artificial Saliva Pump Spray Formulations

The aim of this study was to investigate the rheological behavior and mucoadhesive nature of saliva substitutes, by incorporating various mucoadhesive polymers into an artificial saliva pump spray formulation. For this purpose various mucoadhesive polymers including cellulosic polymers in the range of 0.1-1.0% and Carbomers such as C974p, C971, C934p and C971 in the range of 0.01-0.1% were adde...

متن کامل

The evaluation and comparison of marginal adaptation in metal ceramic and all ceramic restorations fabricated by two methods: CAD/CAM and conventional

Introduction: Marginal fit is a key factor for long term clinical success through any dental restorations. Poor marginal adaptation causes cement dissolution. This can lead to dental caries, gingival irritation, periodontal diseases, and finally treatment failure. The aim of this study was measurement and comparison of marginal gap quantities in metal ceramic and all ceramic dental restorations...

متن کامل

مقایسه تأثیر رستوریشن‌های PFM با رستوریشن‌های All-Ceramic بر تجمع پلاک

  Background and Aims: Tooth crowning often leads to changes in periodontal index through changes in emergence profile zone. The purpose of this study was to compare the effect of metal-ceramic with that ofAll-Ceramic restorations on the plaque a accumulation.   Materials and Methods: In this clinical trial, we used 102 teeth covered with metal-ceramic and all-ceramic restorations. Before and a...

متن کامل

Effect of Zirconia Thickness on the Tensile Stress of Zirconia Based All-Ceramic Restorations

Introduction: The purpose of the presented study was to evaluate the effect of zirconia thickness on the tensile stress of zirconia based all-ceramic restorations. Methods: Twenty zirconia disks with 10mm diameter were prepared in two groups using CAD/CAM system. The thickness of zirconia was 0.5mm in first group and 0.3mm in second group. After sintering, 0.4mm glass ceramic porcelain was appl...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 8  شماره 

صفحات  -

تاریخ انتشار 2015