EXAFS studies of the chemical state of lead and copper in corrosion products formed on the brass surface in potable water.

نویسندگان

  • A I Frenkel
  • G V Korshin
چکیده

EXAFS measurements in the corrosion deposits were performed on Bell Labs-UIUC beamline X16C at the NSLS at Brookhaven National Laboratory in grazing incidence fluorescence mode at room temperature. EXAFS in the reference Cu and Pb metal foils, malachite, cerussite and hydrocerussite were measured in transmission. Sagittally focused second crystal in the double crystal Si (111) monochromator allowed to horizontally focus the beam to the 1 mm size at the sample position. Harmonics were rejected by detuning the monochromator (Si 111) by-20%. Lytle detector was used for fluorescence detection. Ni and Ge filters (3 absorption lengths thick each) were used for Cu K edge and Pb L3 edge XAFS measurements, respectively. Care was taken to ensure that the XAFS signal from corrosion layer only contributes to the total signal. For that, the sample was rotated and XAFS was measured several times and signals were compared until the contribution from the bulk brass vanished. Corrosion products formed on the surface of lead-containing brass were examined using grazing incidence fluorescence EXAFS. The corrosion scales were shown to be comprised by malachite Cux(OH)2CO 3 and hydrocerussite Pb3(OH)2(CO3) 2. The equatorial and axial Cu-O distances in the corrosion deposits were virtually the same as in the reference malachite sample, whereas the disorder in the Cu-O distances in the corrosion products was enhanced. The chemical environment around the Pb atoms in the corrosion deposits was similar to that in hydrocerussite but there was an apparent shortening of the Pb-O nearest neighbor distances in the corrosion deposits compared to those in pure hydrocerussite.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Copper Pitting and Brass Dezincification: Chemical and Physical Effects

OBJECTIVES: The key hypothesis of this project was that both chemical and physical factors associated with real plumbing systems may influence copper pitting and brass dezincification corrosion, and thus the project was aimed at better understanding these factors. In addition to a comprehensive review of the literature on brass dezincification in potable water systems, experimental work was und...

متن کامل

Corrosion and scaling potential of the potable water in villages based on langelier saturation index, ryznar stability index, larson ratio, and saturation level

Abstract Background: corrosion and scaling are of the most important characteristics of drinking water, affecting public health and water industry economy. The aim of the present study was to evaluate the corrosion and scaling potential of potable water supplied by Saqqez Rural Water and Wastewater Company. Materials and Methods: this was a descriptive study conducted on 142 samples taken from ...

متن کامل

Dealloying and Stress Corrosion Craking of Copper Alloys in Cu(I) Solutions

Natural cases of dealloying or stress-corrosion cracking in copper alloys normally occur in oxygenated solutions, where the cathodic reactant is O2 or Cu2+. Within cavities or under deposits, the local environment is enriched in cuprous ions (e.g. CuCl2-, Cu (NH3)2+) and the potential is close to the Cu/Cu+ equilibrium. Such conditions can be simulated macroscopically by stirring powdered Cu2O ...

متن کامل

بررسی روند تشکیل ترکیبات اکسیدی در آثار برنزی با استناد به مطالعات میکروسکوپی

Due to the complex corrosion mechanism of the bronze objects, explaining the structure of different layers of corrosion in these objects at microscopic levels is possible. Typically copper oxide(I) is the first corrosion layer on surface of bronze objects that are excavated of historical sites. However, depending on the environmental conditions، various forms of corrosion layer of tin or copper...

متن کامل

Quantum chemical studies on adsorption of imidazole derivatives as corrosion inhibitors for mild steel in 3.5 NaCl solution

Adsorption of benzimidazole, 2-methylbenzimidazole and 2-aminobenzimidazole on mild steel in 3.5 NaCl solution was studied using density function theory DFT calculations. In this regard, charge transfer resistance Rct and double layer capacitance Cdl obtained by electrochemical impedance spectroscopy EIS were used to calculate surface coverage and to build prediction models. When prediction mod...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of synchrotron radiation

دوره 6 Pt 3  شماره 

صفحات  -

تاریخ انتشار 1999