Microstructure, Pitting Corrosion Resistance and Impact Toughness of Duplex Stainless Steel Underwater Dry Hyperbaric Flux-Cored Arc Welds
نویسندگان
چکیده
Duplex stainless steel multi-pass welds were made at 0.15 MPa, 0.45 MPa, and 0.75 MPa pressure, simulating underwater dry hyperbaric welding by the flux-cored arc welding (FCAW) method, with welds of normal pressure as a benchmark. The purpose of this work was to estimate the effect of ambient pressure on the microstructure, pitting corrosion resistance and impact toughness of the weld metal. The microstructure measurement revealed that the ferrite content in the weld metal made at 0.45 MPa is the lowest, followed by that of 0.75 MPa and 0.15 MPa. The analysis of potentiodynamic polarization tests at 30 °C and 50 °C demonstrated that the pitting corrosion resistance depends on the phases of the lower pitting resistance equivalent numbers (PREN), secondary austenite and ferrite. The weld metal made at 0.45 MPa had the best resistance to pitting corrosion at 30 °C and 50 °C with the highest PRENs of secondary austenite and ferrite. The weld metal made at 0.15 MPa displayed the lowest pitting corrosion resistance at 30 °C with the lowest PREN of secondary austenite, while the weld metal made at 0.75 MPa was the most seriously eroded after being tested at 50 °C for the lowest PREN of ferrite, with large cluster pits seen in ferrite at 50 °C. The impact tests displayed a typical ductile-brittle transition because of the body-centered cubic (BCC) structure of the ferrite when the test temperature was lowered. All the weld metals met the required value of 34 J at -40 °C according to the ASTM A923. The highest ferrite content corresponded to the worst impact toughness, but the highest toughness value did not correspond to the greatest austenite content. With the decreasing of the test temperature, the drop value of absorbed energy was correlated to the ferrite content. Additionally, in this work, the weld metal made at 0.45 MPa had the best combined properties of pitting resistance and impact toughness.
منابع مشابه
The Evaluation of Corrosion Behavior of AISI 347 Stainless Steel to ASTM A335 Low Alloy Steel Dissimilar Welds
In the present study, the corrosion behavior of AISI 347 austenitic stainless steel to ASTM A335 low alloy steel dissimilar joint was investigated. For this purpose, two filler metals, ER309L and ERNiCr-3, were selected to be used during the gas tungsten arc welding process. To investigate the corrosion behavior of the joints after welding, the specimens were tested in 3.5% sodium chloride solu...
متن کاملEvaluation of the corrosion behavior of the base metal and weld metal sections of the super duplex stainless steel UNS S32750
In this study, the corrosion behavior of super duplex stainless steel UNS S32750 and tungsten arc welding with filler metals AWS ER2594 duplex stainless steel in acidic solution containing chloride ions have been investigated. Microstructure of weld joints evaluateby light and electron microscope and corrosion behavior examine by open circuit potential and cyclic polarization tests.The results ...
متن کاملEvaluation of the corrosion behavior of the base metal and weld metal sections of the super duplex stainless steel UNS S32750
In this study, the corrosion behavior of super duplex stainless steel UNS S32750 and tungsten arc welding with filler metals AWS ER2594 duplex stainless steel in acidic solution containing chloride ions have been investigated. Microstructure of weld joints evaluateby light and electron microscope and corrosion behavior examine by open circuit potential and cyclic polarization tests.The results ...
متن کاملCorrosion performance of welds in duplex, superduplex and lean duplex stainless steels
To achieve good corrosion resistance in a weld is much more challenging than for plate or sheet material, which has undergone controlled rolling, heat treatment and pickling processes in the steel mill. The choice of weld procedure and parameters, filler metal and shielding gas all play important roles. For duplex and lean duplex grades it is essential to ensure that an adequate amount of auste...
متن کاملEffect of Annealing Temperature on the Mechanical and Corrosion Behavior of a Newly Developed Novel Lean Duplex Stainless Steel
The effect of annealing temperature (1000-1150 °C) on the microstructure evolution, mechanical properties, and pitting corrosion behavior of a newly developed novel lean duplex stainless steel with 20.53Cr-3.45Mn-2.08Ni-0.17N-0.31Mo was studied by means of optical metallographic microscopy (OMM), scanning electron microscopy (SEM), magnetic force microscopy (MFM), scanning Kelvin probe force mi...
متن کامل