ZT > 0.1 Electron‐Carrying Polymer Thermoelectric Composites with In Situ SnCl2 Microstructure Growth
نویسندگان
چکیده
An n-type pyromellitic diimide polymer composite with in situ microstructure growth of the common element compound SnCl2 reaches power factor of 50-100 μW m-1 K-2, the highest purely n-type polymer composite power factor yet reported. The composite has a gigantic Seebeck coefficient between -4000 and -5000 μV K-1, many times higher than other polymer composites.
منابع مشابه
Synergistic Optimization of Thermoelectric Performance in P-Type Bi0.48Sb1.52Te3/Graphene Composite
We report the synergistic optimization of the thermoelectric properties in p-type Bi0.48Sb1.52Te3 by the additional graphene. Highly dense Bi0.48Sb1.52Te3 + graphene (x wt%, x = 0, 0.05, 0.1 and 0.15) composites have been synthesized by zone-melting followed by spark plasma sintering. With the help of scanning electron microscopy, the graphene has been clearly observed at the edge of the grain ...
متن کاملEnhancing thermoelectric properties of organic composites through hierarchical nanostructures
Organic thermoelectric (TE) materials are very attractive due to easy processing, material abundance, and environmentally-benign characteristics, but their potential is significantly restricted by the inferior thermoelectric properties. In this work, noncovalently functionalized graphene with fullerene by π-π stacking in a liquid-liquid interface was integrated into poly(3,4-ethylenedioxythioph...
متن کاملSynthesis and Thermoelectric Properties of TiO2/Cu2SnSe3 Composites
Thermoelectric (TE) materials are a kind of energy material which can directly convert waste heat into electricity based on TE effects. Ternary Cu2SnSe3 material with diamond-like structure has become one of the potential TE materials due to its low thermal conductivity and adjustable electrical conductivity. In this study, the Cu2SnSe3 powder was prepared by vacuum melting-quenching-annealing-...
متن کاملCarbon fiber polymer–matrix structural composites exhibiting greatly enhanced through-thickness thermoelectric figure of merit
The through-thickness thermoelectric behavior of continuous carbon fiber epoxy-matrix composites is greatly improved by adding tellurium particles (13 vol.%), bismuth telluride particles (2 vol.%) and carbon black (2 vol.%). The thermoelectric power is increased from 8 to 163 lV/K, the electrical resistivity is decreased from 0.17 to 0.02.X.cm, the thermal conductivity is decreased from 1.31 to...
متن کاملThermoelectric Properties of Alumina-Doped Bi0.4Sb1.6Te3 Nanocomposites Prepared through Mechanical Alloying and Vacuum Hot Pressing
In this study, γ-Al2O3 particles were dispersed in p-type Bi0.4Sb1.6Te3 through mechanical alloying to form γ-Al2O3/Bi0.4Sb1.6Te3 composite powders. The composite powders were consolidated using vacuum hot pressing to produce nanoand microstructured composites. Thermoelectric (TE) measurements indicated that adding an optimal amount of γ-Al2O3 nanoparticles improves the TE performance of the fa...