Wear Behavior of Ceramic CAD/CAM Crowns and Natural Antagonists
نویسندگان
چکیده
OBJECTIVE Evaluation of wear behavior of computer-aided design/computer-aided manufacturing (CAD/CAM) crowns from various restorative materials and natural antagonists. METHOD Full CAD/CAM crowns fabricated with nanoceramic resin (Lava Ultimate (LU)), a glass ceramic in a resin interpenetrating matrix (Vita Enamic (VE)) and a lithium silicate reinforced ceramic enriched with zirconia (Vita Suprinity (VS)) were cemented on human molars. The crown and antagonists were subjected to simulated chewing. 3D data sets, before and after the chewing simulation, were generated and matched. Occlusal surface roughness, vertical and volume loss of the crowns and antagonists were analyzed. RESULTS Crown roughness was significantly different between the LU and VE groups after chewing simulation. Crown vertical loss differed in all groups. The highest crown volume loss was found in the LU group, and the lowest in the VE group. Comparisons between the LU and VE groups and the LU and VS groups were significantly different. The highest antagonist volume loss was reached in the VE group, the lowest was in the LU group. CONCLUSION Roughness increased after chewing simulation. LU crowns are the most natural antagonist-friendly; these were the most susceptible to vertical and volume loss. Of the tested materials, the VE crowns are the most stable regarding occlusion.
منابع مشابه
The Effect of Different Finishing Lines on the Marginal Fitness of Full Contour Zirconia and Glass Ceramic CAD/CAM Crowns (An in-vitro study)
Purpose: The aim of this study was to evaluate the effect of two gingival finishing lines (90° shoulder and deep chamfer) on the marginal fitness of two types of full anatomic all-ceramic crowns; zirconia crowns (Zikonzhan) and glass ceramic crowns (IPS e-max CAD) milled with CAD/CAM system. Materials and Methods: Two dentoform teeth of left maxillary first molar were prepared with chamfer fini...
متن کاملTwo-body wear rate of CAD/CAM resin blocks and their enamel antagonists.
STATEMENT OF PROBLEM Computer-aided design and computer-aided manufacturing (CAD/CAM) resins exhibit good mechanical properties and can be used as long-term restorations. The wear rate of such resins and their enamel antagonists is unknown. PURPOSE The purpose of this study was to test and compare the 2-body wear rate of CAD/CAM resin blocks. MATERIAL AND METHODS Wear specimens (N=42, n=6) ...
متن کاملComparative fracture strength analysis of Lava and Digident CAD/CAM zirconia ceramic crowns
PURPOSE All-ceramic crowns are subject to fracture during function. To minimize this common clinical complication, zirconium oxide has been used as the framework for all-ceramic crowns. The aim of this study was to compare the fracture strengths of two computer-aided design/computer-aided manufacturing (CAD/CAM) zirconia crown systems: Lava and Digident. MATERIALS AND METHODS Twenty Lava CAD/...
متن کاملCAD/CAM-titanium-ceramic single crowns with non-anatomic coping-design. A six-year follow-up study
Objectives Due to the increasing price of gold CAD/CAM titanium-ceramic restorations were developed to give alternative to the established metal-ceramic restorations with a high gold content. Despite the advantages of excellent biocompatibility, high corrosion resistance and appropriate strength titanium has made the casting process difficult caused by the high affinity of molten titanium to in...
متن کاملEvaluation of marginal fit of 2 CAD-CAM anatomic contour zirconia crown systems and lithium disilicate glass-ceramic crown
PURPOSE This study was to evaluate the marginal fit of two CAD-CAM anatomic contour zirconia crown systems compared to lithium disilicate glass-ceramic crowns. MATERIALS AND METHODS Shoulder and deep chamfer margin were formed on each acrylic resin tooth model of a maxillary first premolar. Two CAD-CAM systems (Prettau®Zirconia and ZENOSTAR®ZR translucent) and lithium disilicate glass ceramic...
متن کامل