Numerical Study of Liquid Phase Hydrogen Peroxide Decomposition in Catalytic Micro-reactors
نویسندگان
چکیده
Hydrogen peroxide has recently been considered as a monopropellant in micropropulsion systems for the next generation of miniaturized satellites (‘nanosats’) due to its high energy density, modest specific impulse and “green” characteristics. Efforts at the University of Vermont have focused on the development of a MEMS-based microthruster that uses the catalyzed decomposition of hydrogen peroxide to generate thrust and impulse-bits commensurate with the intended micropropulsion application. The present study is a computational effort to investigate the initial decomposition of the monopropellant as it enters a catalytic chamber. Two-dimensional numerical models of the monopropellant in microchannel geometry have been developed and used to characterize the performance of the monopropellant before vaporization occurs. The results of these studies show that in the absence of a non-diffusive mixing mechanism at the microscale, decomposition of the monopropellant occurs very slowly. A method for enhancing decomposition via the introduction of gas bubbles into the flow is studied, and found to increase decomposition for a given length by over 57%.
منابع مشابه
Catalytic Decomposition of Hydrogen Peroxide in the Presence of Synthesized Iron-Manganese oxide Nanocomposites via Different Methods
The special application of iron-manganese oxide nanocatalysts has been investigated in decomposition of hydrogen peroxide. In this research, iron-manganese oxide nanocomposites were synthesized by co-precipitation, sol-gel and mechanochemical methods using iron (III) nitrate, iron (II) sulfate and manganese (II) nitrate as starting materials. These nanocomposites were prepared on the variou...
متن کاملPreparation of Promoted Ni0.1Co0.9Fe2O4 Ferrite Nanoparticles and Investigation of Its Catalytic Activity on Decomposition of H2O2 and Optical Characterization of Pure Ni0.1Co0.9Fe2O4
Pure and ZnO-doped Ni0.1Co0.9Fe2O4 catalyst were prepared by co-precipitation method and thermal decomposition in air calcinated at 400-700°C and that treated with different amounts of zinc nitrate (0.46-2.25 w% ZnO). X-ray powder diffractometry, scanning electron microscopy (SEM) and BET analysis of nitrogen adsorption isotherms investigated the crystalline bulk structure and the surface area ...
متن کاملCatalytic Decomposition of H2O2 on MnFe2O4 Nanocomposites Synthesized by Various Methods in the Presence of Silicate and Zeolite Supports
In this research iron manganese oxide nanocomposites were prepared by co-precipitation, sol-gel and mechanochemical methods by using iron (III) nitrate, iron (II) sulfate and manganese (II) nitrate as starting materials. These nanocomposites were prepared in the presence of various catalyst beds. The polyvinyl pyrrolidon (PVP) was used as a capping agent to control the agglomeration of the nano...
متن کاملPreparation of Promoted Ni0.1Co0.9Fe2O4 Ferrite Nanoparticles and Investigation of Its Catalytic Activity on Decomposition of H2O2 and Optical Characterization of Pure Ni0.1Co0.9Fe2O4
Pure and ZnO-doped Ni0.1Co0.9Fe2O4 catalyst were prepared by co-precipitation method and thermal decomposition in air calcinated at 400-700°C and that treated with different amounts of zinc nitrate (0.46-2.25 w% ZnO). X-ray powder diffractometry, scanning electron microscopy (SEM) and BET analysis of nitrogen adsorption isotherms investigated the crystalline bulk structure and the surface area ...
متن کاملCharacterization of Cobalt Oxide Co3O4 Nanoparticles Prepared by Various Methods: Effect of Calcination Temperatures on Size, Dimension and Catalytic Decomposition of Hydrogen Peroxide
In this scientific research work we report a novel method to synthesis Co3O4 nanoparticles via calcinations of cobalt hydroxide which can be conveniently prepared by the Co(NO3 )2.6H2O with different reactants. In order to study the effect of calcination temperature on structure and morphology of the nanoparticles, the calcinations take place at various temperatures (at 300°C, 500°C and 700°C)....