OBJECTIVE This study was aimed to evaluate and to compare the push-out bond strength of different brands of mineral trioxide aggregate (MTA) with a calcium enriched mixture cement (CEM). MATERIALS AND METHODS Fifteen extracted, single-rooted human teeth were used. The middle-third of the roots were sliced perpendicular to the long axis into 1.00 ± 0.05 mm thick serial slices (15 root × 4 slice = 60 specimen). The specimens were then divided into three groups (n = 20). The standardized root discs were filled with white CEM, ProRoot MTA, MTA-Angelus and wrapped in a serum-soaked gauze. After 3 days at relative humidity, the push-out bond strengths were measured with a universal testing machine. Data were analyzed using one-way analysis of variance and post hoc Tukey tests. RESULTS The mean push-out bond strength value of the ProRoot MTA group (12.7 ± 2.5 MPa) was the highest and statistically significant difference was recorded between ProRoot MTA and other groups (P < 0.001). There was no significant difference between the mean bond strength of CEM cement (4.6 ± 1.1 MPa) and MTA-Angelus (4.5 ± 1.5 MPa) (P = 0.982). CONCLUSION The push-out bond strength of MTA was changed with the brands and ProRoot MTA had the highest push-out bond strength.
منابع مشابه
Bond Strength of White Mineral Trioxide Aggregate with and without Disodium Hydrogen Phosphate with Different Liquid-to-Powder Ratios
INTRODUCTION Mineral trioxide aggregate (MTA) can be used in the treatment of irritated vital pulp and repair of root perforations. However, the initial reaction of inflammatory cells to this material and also its setting time are not ideal. Studies have shown that disodium hydrogen phosphate (DHP), decreases the setting time of MTA, with no effect on its pH. This study was undertaken to evalua...
متن کاملComparison of bond strength of different endodontic sealers to root dentin: An in vitro push-out test
AIM To compare the bond strength of four different endodontic sealers to root dentin through push-out test design. MATERIALS AND METHODS Forty single-rooted teeth with completely formed apices were selected. Teeth were decoronated, and working length was determined. Instrumentation and irrigation were performed. The teeth were divided into four groups based upon the sealer used. Group 1: Bioc...
متن کاملComparison of push-out bond strength of mineral trioxide aggregate and calcium enriched mixture cement as root end filling materials
BACKGROUND The purpose of this study was to compare the push-out bond strength of mineral trioxide aggregate (MTA) and calcium enriched mixture (CEM) as root end filling materials. MATERIALS AND METHODS A total of 40 root dentin slices (1 ± 0.2 mm) were prepared from freshly extracted human maxillary central teeth and their lumens were enlarged to 1.3 mm. The slices were randomly divided into...
متن کاملThe Effect of Calcium Chloride on Push-Out Bond Strength of Calcium-Enriched Mixture Cement and Mineral Trioxide Aggregate
INTRODUCTION This in vitro study investigated the effect of adding 10% calcium chloride (CaCl2) on push out bond strength of calcium-enriched mixture (CEM) cement and mineral trioxide aggregate (MTA) to root canal dentin. METHODS AND MATERIALS A total of 120 root dentin slices with 2 mm thickness were prepared from sixty single-rooted human teeth. Dentinal discs were enlarged to achieve 1.3 m...
متن کاملEffect of the TiO2 nanoparticles on the selected physical properties of mineral trioxide aggregate
BACKGROUND Some of the efforts to improve the properties of Mineral Trioxide Aggregate (MTA) include incorporation of some nanoparticles such as Titanium dioxide (TiO2). The aim of this study was to evaluate the effect of TiO2 nanoparticles on the setting time, working time, push-out bond strength and compressive strength of MTA. MATERIAL AND METHODS The physical properties to be evaluated we...
متن کامل