Kinetics and fracture resistance of lithiated silicon nanostructure pairs controlled by their mechanical interaction
نویسندگان
چکیده
Following an explosion of studies of silicon as a negative electrode for Li-ion batteries, the anomalous volumetric changes and fracture of lithiated single Si particles have attracted significant attention in various fields, including mechanics. However, in real batteries, lithiation occurs simultaneously in clusters of Si in a confined medium. Hence, understanding how the individual Si structures interact during lithiation in a closed space is necessary. Here, we demonstrate physical and mechanical interactions of swelling Si structures during lithiation using well-defined Si nanopillar pairs. Ex situ SEM and in situ TEM studies reveal that compressive stresses change the reaction kinetics so that preferential lithiation occurs at free surfaces when the pillars are mechanically clamped. Such mechanical interactions enhance the fracture resistance of lithiated Si by lessening the tensile stress concentrations in Si structures. This study will contribute to improved design of Si structures at the electrode level for high-performance Li-ion batteries.
منابع مشابه
High damage tolerance of electrochemically lithiated silicon
Mechanical degradation and resultant capacity fade in high-capacity electrode materials critically hinder their use in high-performance rechargeable batteries. Despite tremendous efforts devoted to the study of the electro-chemo-mechanical behaviours of high-capacity electrode materials, their fracture properties and mechanisms remain largely unknown. Here we report a nanomechanical study on th...
متن کاملKinetics of initial lithiation of crystalline silicon electrodes of lithium-ion batteries.
Electrochemical experiments were conducted on {100}, {110}, and {111} silicon wafers to characterize the kinetics of the initial lithiation of crystalline Si electrodes. Under constant current conditions, we observed constant cell potentials for all orientations, indicating the existence of a phase boundary that separates crystalline silicon from the amorphous lithiated phase. For a given poten...
متن کاملThermal Stress Resistance to Fracture and its Relation to with Resistance to Thermal Fatigue and Shock
Dense Silicon nitride was investigated to determine the effect of its microstructural parameters and densification on thermo-mechanical properties and thermal stress resistance to fracture initiation during a hot or cold mechanical and thermal shock testing. The different materials and microstructures were obtained by changing the parameters such as the type of the powder, additive, forming p...
متن کاملRobustness of amorphous silicon during the initial lithiation/delithiation cycle
Recent research on the electrochemical lithiation of amorphous silicon nanoparticles shows that amorphous silicon is more fracture resistant than crystalline silicon during lithiation. Nanoparticles of amorphous silicon can be lithiated and delithiated without any fracture at all. To fully exploit the potential of using amorphous silicon as electrodes for lithium ion batteries it is important t...
متن کاملThermal Stress Resistance to Fracture and its Relation to with Resistance to Thermal Fatigue and Shock
Dense Silicon nitride was investigated to determine the effect of its microstructural parameters and densification on thermo-mechanical properties and thermal stress resistance to fracture initiation during a hot or cold mechanical and thermal shock testing. The different materials and microstructures were obtained by changing the parameters such as the type of the powder, additive, forming p...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
عنوان ژورنال:
دوره 6 شماره
صفحات -
تاریخ انتشار 2015