Influence of the grain size on the in vivo degradation behaviour of the magnesium alloy LAE442.

نویسندگان

  • Berit Ullmann
  • Janin Reifenrath
  • Jan-Marten Seitz
  • Dirk Bormann
  • Andrea Meyer-Lindenberg
چکیده

The aim of this study was to investigate the differences in the in vivo degradation behaviour of magnesium implants with various grain sizes and damaged surfaces. For this purpose, three different LAE442 magnesium implants were produced: cast, single and double extruded implants, in order to obtain different grain sizes. Furthermore, defects were positioned on the surfaces of some of the single extruded implants. The initial stability was determined. Four pins of each implant material were implanted into rabbits' tibiae and regularly clinically, radiologically and micro-computed tomographically investigated over a period of 27 weeks. Following explantation, investigations were carried out using stereo and scanning electron microscopy including energy-dispersive X-ray analyses. Weight and strength changes were measured. The double extruded implants possessing the finest grains exhibited the highest initial stability (179.18 N). These implants demonstrated the lowest in vivo corrosion rates (0.0134 mm/year) and the least radiologically visible changes. The highest corrosion rate was computed for the implants possessing damaged surfaces. Radiologically discernible bone changes occurred at almost the same time as implant changes for all groups. Based on these results, the aim should be to produce fine-grained magnesium-based alloys for resorbable implants and to avoid any surface damage.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

In Vivo Degradation Behavior of the Magnesium Alloy LANd442 in Rabbit Tibiae

In former studies the magnesium alloy LAE442 showed promising in vivo degradation behavior and biocompatibility. However, reproducibility might be enhanced by replacement of the rare earth composition metal "E" by only a single rare earth element. Therefore, it was the aim of this study to examine whether the substitution of "E" by neodymium ("Nd") had an influence on the in vivo degradation ra...

متن کامل

The influence of storage and heat treatment on a magnesium-based implant material: an in vitro and in vivo study

BACKGROUND Magnesium alloys are recommended as a potential material for osteosynthesis. It is known that storage-induced property modifications can occur in materials like aluminum. Thus the aim of this study was to analyze the influence of storage durations of up to 48 weeks on the biomechanical, structural, and degradation properties of the degradable magnesium alloy LAE442. METHODS Extrude...

متن کامل

Influence of Heat Treatment on the Degradation Behaviour of Degradable Magnesium Based Implants.

Aim of the study was to characterise the influence of heat treatment on the degradation behaviour and stability of degradable magnesium based implants. For this purpose two groups (untreated/ heat treated) of LAE442 pins were separately analysed in an in vitro and in vivo study. The corrosion behaviour was evaluated during 8 weeks degradation in SBF (in vitro) and 48 weeks degradation intramedu...

متن کامل

Mechanical Behavior of an Ultrafine/Nano Grained Magnesium Alloy

The application of magnesium alloys is greatly limited because of their relatively low strength and ductility. An effective way to improve the mechanical properties of magnesium alloy is to refine the grains. As the race for better materials performance is never ending, attempts to develop viable techniques for microstructure refinement continue. Further refining of grain size requires, however...

متن کامل

Grain Refinement and Enhancement of Mechanical Properties of Hot Extruded Rare-Earth Containing Magnesium Alloy

The effects of rare earth addition and hot extrusion process on the grain refinement of magnesium alloy were studied. The as-cast Mg-6Al-1Zn (AZ61) alloy had the average grain size of ~ 64 µm and its microstructure consisted of α-Mg and Mg17Al12 phase. By partial substitution of Al with Gd to reach Mg-4.8Gd-1.2Al-1Zn alloy, it was observed that the Mg17Al12 phase disappeared and two new interme...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Proceedings of the Institution of Mechanical Engineers. Part H, Journal of engineering in medicine

دوره 227 3  شماره 

صفحات  -

تاریخ انتشار 2013