Shear bond strength of indirect composite material to monolithic zirconia
نویسندگان
چکیده
PURPOSE This study aimed to evaluate the effect of surface treatments on bond strength of indirect composite material (Tescera Indirect Composite System) to monolithic zirconia (inCoris TZI). MATERIALS AND METHODS Partially stabilized monolithic zirconia blocks were cut into with 2.0 mm thickness. Sintered zirconia specimens were divided into different surface treatment groups: no treatment (control), sandblasting, glaze layer & hydrofluoric acid application, and sandblasting + glaze layer & hydrofluoric acid application. The indirect composite material was applied to the surface of the monolithic zirconia specimens. Shear bond strength value of each specimen was evaluated after thermocycling. The fractured surface of each specimen was examined with a stereomicroscope and a scanning electron microscope to assess the failure types. The data were analyzed using one-way analysis of variance (ANOVA) and Tukey LSD tests (α=.05). RESULTS Bond strength was significantly lower in untreated specimens than in sandblasted specimens (P<.05). No difference between the glaze layer and hydrofluoric acid application treated groups were observed. However, bond strength for these groups were significantly higher as compared with the other two groups (P<.05). CONCLUSION Combined use of glaze layer & hydrofluoric acid application and silanization are reliable for strong and durable bonding between indirect composite material and monolithic zirconia.
منابع مشابه
Micro-Shear Bond Strength of Indirect Composite Resin to Three Different Computer-Milled Cores After Thermocycling
Background and Aim: The aim of this study was to evaluate the micro-shear bond strength of an indirect composite resin to three different types of cores. Materials and Methods: In this in-vitro study, 14 blocks (5×5×2 mm) were designed and milled by computer from cobalt-chromium (Co-Cr) alloy, zirconia, and polyether ether ketone (PEEK). Each sample was treated according to the manufacturer’s ...
متن کاملEffect of surface treatment on bond strength between an indirect composite material and a zirconia framework.
The present study evaluated the effect of various surface treatments for zirconia ceramics on shear bond strength between an indirect composite material and zirconia ceramics. In addition, we investigated the durability of shear bond strength by using artificial aging (20,000 thermocycles). A total of 176 Katana zirconia disks were randomly divided into eight groups according to surface treatme...
متن کاملShear bond strength between an indirect composite veneering material and zirconia ceramics after thermocycling.
The present study evaluated the shear bond strength between an indirect composite material and zirconium dioxide (zirconia) ceramics after thermocycling. A total of 80 zirconia (Katana) discs were divided into five groups and primed with one of following agents: All Bond 2 Primer B (ABB), Alloy Primer (ALP), AZ Primer (AZP), Estenia Opaque Primer (EOP), and Porcelain Liner M Liquid A (PLA). An ...
متن کاملInfluence of 10-MDP Adhesive System on Shear Bond Strength of Zirconia-Composite Interfaces
Introduction: This in-vitro study investigated the initial 24h bond strength between different composites and zirconia after application of four different adhesive systems. Methods: A total of 120 specimens of zirconia (InCoris, Sirona, Germany, Bernsheim) were ground with a 165 µm grit rotating diamond disc. Thirty specimens were each additionally treated with Cimara Zircon “CZ” (VOCO GmbH, ...
متن کاملIn Vitro Effects of Different Surface Preparation Techniques on Shear Bond Strength of Direct to Indirect Composite Resin
Objective: Repair of an indirect restoration is usually preferred over its replacement. This study aimed to evaluate the effect of silane in different surface preparation techniques on the bond strength of direct to indirect composite resin. Methods: For this in vitro experimental study, 48 indirect composite cubes were fabricated, divided into 4 groups of 12 and subjected to the following ...