Maintenance of stellite and tungsten carbide saw tips: respiratory health and exposure-response evaluations.
نویسندگان
چکیده
OBJECTIVE To study exposure to cobalt and chromium in saw maintenance rooms and test respiratory health among saw filers at lumber mills. Hard-metal lung disease is associated with cobalt in the manufacture of tungsten carbide tools; recently it has also been reported among tool maintenance workers. Lumber mills often use saws tipped with tungsten carbide or with a newer alloy, stellite (containing more cobalt, as well as chromium). METHODS A cross sectional study of 118 saw filers at eight lumber mills was carried out that included a standardised questionnaire, spirometry, personal air sampling, and examination of tasks every 10 minutes (by observation). Comparison data were from a study of bus mechanics tested with similar methods. RESULTS AND CONCLUSION Cobalt exposure was associated with tungsten carbide grinding but not with stellite grinding. Chromium exposure was associated mainly with stellite welding. Saw filers had a twofold increase in phlegm and wheeze (P < 0.01) and a threefold increase in cough, phlegm, and wheeze related to work (P < 0.001), but no increase in breathlessness. Stellite welding was associated with a significant increase in nasal symptoms and cough related to work and a small decrease in airflow (forced expiratory volume in one second/forced vital capacity (FEV1/FVC%), P < 0.05). Saw filers wet grinding with tungsten carbide had significant reductions in forced expiratory lung volumes (FEV1 and FVC, P < 0.05) and were significantly more likely to have FEV1 and FVC values in the abnormal range. Cobalt exposure (in wet grinding) and duration of work that involved tungsten carbide grinding were both associated with significant reductions in FEV1 and FVC. Average cobalt exposures in this study were about 5 micrograms/m3, well below the currently accepted permissible concentration, which suggests that the current workplace limit for cobalt may be too high.
منابع مشابه
Cladding of stellite composite on carbon steel by gas tungsten arc welding (GTAW)
This paper deals with the investigation of the microstructure and hardness of steel samples cladded with satellite 6-WC composites by using gas tungsten arc welding (GTAW) process. For this purpose, steel samples were coated with unreinforced and reinforced stellite (by 20, 30 and 40 wt.% WC). The cladded samples were evaluated by metallographic studies, microhardness measurement and X-ray diff...
متن کاملSpecific Fast Response CH4 Gas Sensor Based on Metal Oxide, Tungsten Carbide /SnO2Core-Shell Modified Interdigitated Electrode
In this study, a specific CH4 sensor is fabricated based on interdigitated electrode that modified with core-shell of tungsten carbide/tin oxide (WC/SnO2) nanoparticles by wet chemical method in different percents of carbon and tungsten. The morphology of wet chemical-synthesized WC/SnO2 core-shell was evaluated by different methods such as patterned X-ray d...
متن کاملOccupational exposure to welding gases during three welding processes and risk assessment by SQRCA method
Background: Hazardous chemical agents in the welding operation are a mixture of metal fumes and toxic gases, the inhalation of which causes adverse health effects among welders. The emission of gases in the workplace is a logical cause for concern regarding the potential development of respiratory disease. The aim of the present study was to determine the concentration values of gases discharge...
متن کاملCharacterization of tungsten tips for STM by SEM/AES/XPS
For the first time, both X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES) techniques were applied in analysis of surface contamination of electrochemically etched Scanning Tunneling Microscope (STM) tungsten tips. Carbon monoxide, graphite, tungsten carbide and tungsten oxide were found as main surface contaminations of STM tungsten tips. The thickness of tungsten ox...
متن کاملEnamel surface evaluation after bracket debonding and different resin removal methods
OBJECTIVE To assess enamel surface under scanning electron microscopy (SEM) after resin removal and enamel polishing procedures following brackets debonding, as well as compare the time required for these procedures. METHODS A total of 180 deciduous bovine incisors were used. The enamel surface of each tooth was prepared and brackets were bonded with light cured Transbond XT composite resin. ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Occupational and environmental medicine
دوره 52 3 شماره
صفحات -
تاریخ انتشار 1995