Microtensile bond strength of a repair composite to leucite-reinforced feldspathic ceramic.

نویسندگان

  • Renata Marques de Melo
  • Luiz Felipe Valandro
  • Marco Antonio Bottino
چکیده

The purpose of this study was to evaluate the microtensile bond strength of a repair composite resin to a leucite-reinforced feldspathic ceramic (Omega 900, VITA) submitted to two surface conditionings methods: 1) etching with hydrofluoric acid + silane application or 2) tribochemical silica coating. The null hypothesis is that both surface treatments can generate similar bond strengths. Ten ceramic blocks (6x6x6 mm) were fabricated and randomly assigned to 2 groups (n=5), according to the conditioning method: G1- 10% hydrofluoric acid application for 2 min plus rinsing and drying, followed by silane application for 30 s; G2- airborne particle abrasion with 30 microm silica oxide particles (CoJet-Sand) for 20 s using a chairside air-abrasion device (CoJet System), followed by silane application for 5 min. Single Bond adhesive system was applied to the surfaces and light cured (40 s). Z-250 composite resin was placed incrementally on the treated ceramic surface to build a 6x6x6 mm block. Bar specimens with an adhesive area of approximately 1 +/- 0.1 mm(2) were obtained from the composite-ceramic blocks (6 per block and 30 per group) for microtensile testing. No statistically significant difference was observed between G1 (10.19 +/- 3.1 MPa) and G2 (10.17 +/- 3.1 MPa) (p=0.982) (Student's t test; á = 0.05). The null hypothesis was, therefore, accepted. In conclusion, both surface conditioning methods provided similar microtensile bond strengths between the repair composite resin and the ceramic. Further studies using long-term aging procedures should be conducted.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The effect of different surface treatments on bond strength between leucite reinforced feldspathic ceramic and composite resin.

OBJECTIVES The aim of this study was to evaluate the effect of different surface treatments on the microtensile bond strength between a leucite reinforced glass-ceramic and composite resin. METHODS Leucite reinforced ceramic blocks (n=24) were constructed using the hot pressing technique. The blocks were assigned to 4 groups, which received the following surface treatments: G1: hydrofluoric (...

متن کامل

Effects of surface-conditioning methods on shear bond strength of brackets bonded to different all-ceramic materials.

The aims of this study were to investigate the effects of two surface-conditioning methods on the shear bond strength (SBS) of metal brackets bonded to three different all-ceramic materials, and to evaluate the mode of failure after debonding. Twenty feldspathic, 20 fluoro-apatite, and 20 leucite-reinforced ceramic specimens were examined following two surface-conditioning methods: air-particle...

متن کامل

Bond strength durability of a resin composite on a reinforced ceramic using various repair systems.

OBJECTIVES This study compared the durability of repair bond strength of a resin composite to a reinforced ceramic after three repair systems. METHODS Alumina-reinforced feldspathic ceramic blocks (Vitadur-alpha) (N=30) were randomly divided into three groups according to the repair method: PR-Porcelain Repair Kit (Bisco) [etching with 9.5% hydrofluoric acid+silanization+adhesive]; CJ-CoJet R...

متن کامل

Effect of the Etching Duration and Ultrasonic Cleaning on Microtensile Bond Strength Between Feldspathic Ceramic and Resin Cement

This study assessed the effect of different etching time of hydrofluoric acid and ultrasonic cleaning of the etched ceramic surface on the resin microtensile bond strength stability to a feldspathic ceramic. The research hypotheses investigated were: (1) different etching time does not affect the adhesion resistance; (2) ultrasonic cleaning improves the adhesion resistance. Forty-eight (48) blo...

متن کامل

Microtensile Bond Strength of Three Restorative Core Materials with IPS e.max Press Ceramic by Two Resin Cements

Objectives: The aim of this study was to compare the microtensile bond strengths (µ TBS) of three core materials with one lithium disilicate reinforced ceramic using two resin cements. Methods: Three core materials (Nulite F® (Biodental Technologies), Filtek Z250® (3M-ESPE), Prettau-Anterior® (Zirkonzhan, Germany)) were prepared as blocks (10×10×4 mm3) according...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 18 4  شماره 

صفحات  -

تاریخ انتشار 2007